MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Hexene, Film Grade

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.910 - 0.942 g/cc0.0329 - 0.0340 lb/in³Average value: 0.920 g/cc Grade Count:179
Thickness 8.00 - 120 microns0.315 - 4.72 milAverage value: 28.0 microns Grade Count:95
Melt Flow 0.200 - 19.0 g/10 min0.200 - 19.0 g/10 minAverage value: 1.53 g/10 min Grade Count:179
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 5.38 - 19.3 MPa780 - 2800 psiAverage value: 10.6 MPa Grade Count:99
Film Tensile Strength at Yield, TD 4.48 - 24.1 MPa650 - 3500 psiAverage value: 10.9 MPa Grade Count:99
Tensile Strength, Yield 10.3 - 18.6 MPa1500 - 2700 psiAverage value: 15.2 MPa Grade Count:3
Film Elongation at Break, MD 280 - 1320 %280 - 1320 %Average value: 552 % Grade Count:168
Film Elongation at Break, TD 560 - 6500 %560 - 6500 %Average value: 785 % Grade Count:168
Film Elongation at Yield, MD 19.0 - 43.0 %19.0 - 43.0 %Average value: 27.5 % Grade Count:4
Film Elongation at Yield, TD 12.0 - 36.0 %12.0 - 36.0 %Average value: 18.8 % Grade Count:4
Elongation at Break 600 - 690 %600 - 690 %Average value: 647 % Grade Count:3
Flexural Modulus 0.152 - 0.725 GPa22.0 - 105 ksiAverage value: 0.322 GPa Grade Count:7
Secant Modulus, MD 0.0896 - 0.538 GPa13.0 - 78.0 ksiAverage value: 0.210 GPa Grade Count:128
Secant Modulus, TD 0.0965 - 0.758 GPa14.0 - 110 ksiAverage value: 0.243 GPa Grade Count:128
Puncture Energy 0.791 - 5.31 J0.583 - 3.92 ft-lbAverage value: 3.28 J Grade Count:36
Coefficient of Friction 0.100 - 1.000.100 - 1.00Average value: 0.541 Grade Count:57
Elmendorf Tear Strength MD 10.0 - 680 g10.0 - 680 gAverage value: 254 g Grade Count:92
Elmendorf Tear Strength TD 30.0 - 920 g30.0 - 920 gAverage value: 580 g Grade Count:92
Elmendorf Tear Strength, MD 1.00 - 25.5 g/micron25.4 - 648 g/milAverage value: 11.7 g/micron Grade Count:95
Elmendorf Tear Strength, TD 12.0 - 45.3 g/micron305 - 1150 g/milAverage value: 26.7 g/micron Grade Count:94
Dart Drop 2.20 - 23.6 g/micron56.0 - 600 g/milAverage value: 7.04 g/micron Grade Count:80
Dart Drop Test 49.0 - 1000 g0.108 - 2.20 lbAverage value: 301 g Grade Count:124
Film Tensile Strength at Break, MD 25.5 - 75.1 MPa3700 - 10900 psiAverage value: 49.7 MPa Grade Count:168
Film Tensile Strength at Break, TD 20.0 - 66.9 MPa2900 - 9700 psiAverage value: 39.5 MPa Grade Count:168
Heat Seal Strength Initiation Temperature 101 - 110 °C214 - 230 °FAverage value: 103 °C Grade Count:6
 
Thermal PropertiesMetricEnglishComments
Melting Point 46.1 - 128 °C115 - 262 °FAverage value: 118 °C Grade Count:76
Vicat Softening Point 93.9 - 119 °C201 - 246 °FAverage value: 105 °C Grade Count:42
Brittleness Temperature -70.0 °C-94.0 °FAverage value: -70.0 °C Grade Count:15
 
Optical PropertiesMetricEnglishComments
Haze 1.00 - 30.4 %1.00 - 30.4 %Average value: 12.3 % Grade Count:148
Gloss 9.00 - 150 %9.00 - 150 %Average value: 65.6 % Grade Count:139
Transmission, Visible 90.0 %90.0 %Average value: 90.0 % Grade Count:8
 
Processing PropertiesMetricEnglishComments
Processing Temperature 180 - 270 °C356 - 518 °FAverage value: 222 °C Grade Count:21
Melt Temperature 195 - 270 °C383 - 518 °FAverage value: 220 °C Grade Count:41
Die Opening 0.0640 - 0.280 cm0.0252 - 0.110 inAverage value: 0.138 cm Grade Count:22

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CHT Group QSil 229 Transparent, Liquid Silicone Rubber
CHT Group QSil 223 Transparent, Liquid Silicone Rubber
CHT Group QSil 222 Transparent, Liquid Silicone Rubber
CHT Group QSil 220 Transparent, Liquid Silicone Rubber
CHT Group QSil 219 Transparent, Liquid Silicone Rubber

O3871 / 78263

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.