MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Barlog Plastics KEBALLOY ECO R-PET E302 100% PET recycled
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Unreinforced

Material Notes: KEBALLOY ECO R-PET E302 is a recycled, low-viscosity PET (polyethylene terephthalate) grade approved for direct food applications with improved flowability. The material is supplied as crystallized granules and has an optimized bluish color. This grade is produced from 100% post-consumer bottle flakes.

Properties: amorphous, dimensionally stable, Thin wall thicknesses, compliant for food contact (according to 10/2011 EC), easy flow, semi-crystalline, approved for food contact (EU and FDA)

Typical areas of application: Glasses frames, Cover, Filter cups, Housing, Crockery and cutlery, industrial goods, Cosmetic packaging, Food packaging, Toys, Sports & Leisure Articles

Industries: Household appliances, Industry, Agriculture, Food processing industry, Sanitary industry, Sports & Recreation

Information provided by BARLOG plastics GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.39 g/cc0.0502 lb/in³ISO 1183-1
Melt Flow 41.0 g/10 min
@Load 2.16 kg,
Temperature 285 °C
41.0 g/10 min
@Load 4.76 lb,
Temperature 545 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 55.0 MPa7980 psiISO 527-1
Elongation at Break 100 %100 %ISO 527-1
Modulus of Elasticity 2.50 GPa363 ksiISO 527-1
Charpy Impact Unnotched 10.0 J/cm²47.6 ft-lb/in²ISO 179-1eU
Charpy Impact, Notched 0.350 J/cm²1.67 ft-lb/in²ISO 179-1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 255 °C491 °FISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 68.0 °C154 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 61.0 °C142 °FISO 75-1/-2
Vicat Softening Point 74.0 °C165 °F50°C/h, 50N; DIN EN ISO 306
 
Processing PropertiesMetricEnglishComments
Processing Temperature 280 - 290 °C536 - 554 °Fhot runner
Melt Temperature 270 - 300 °C518 - 572 °F
Mold Temperature <= 20.0 °C<= 68.0 °F
Drying Temperature 160 °C320 °F
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hour
Moisture Content <= 0.00500 %<= 0.00500 %
Back Pressure 4.00 - 8.00 MPa580 - 1160 psi
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBARLO668 / 326742

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.