  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Mapal Plastics Maplon Type H Polypropylene Sheet
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Sheet/Thermoforming Grade

Material Notes: Properties : Good resistance to low temperatures, Moderate stress whitening, Suitable for die cutting, Corona treated on both sides for offset and screen printing.

Applications : Stationery, Printing and packaging products, Industrial applications where low temperature resistance is required

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.910 g/cc0.910 g/cc
Thickness 1000 microns39.4 mil
Surface Tension >= 48 dynes/cm>= 48 dynes/cmSpecial grade can be treated for more than year for offset printing
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 29.0 MPa
@Temperature 23.0 °C
4210 psi
@Temperature 73.4 °F
ASTM D638
Film Tensile Strength at Yield, TD 25.0 MPa
@Temperature 23.0 °C
3630 psi
@Temperature 73.4 °F
ASTM D638
Film Elongation at Break, MD >= 200 %
@Temperature 23.0 °C
>= 200 %
@Temperature 73.4 °F
ASTM D638
Film Elongation at Break, TD >= 100 %
@Temperature 23.0 °C
>= 100 %
@Temperature 73.4 °F
ASTM D638
Film Elongation at Yield, MD 18 %
@Temperature 23.0 °C
18 %
@Temperature 73.4 °F
ASTM D638
Film Elongation at Yield, TD 14 %
@Temperature 23.0 °C
14 %
@Temperature 73.4 °F
ASTM D638
Modulus of Elasticity 0.400 GPa
@Temperature 23.0 °C
58.0 ksi
@Temperature 73.4 °F
MD/TD; ASTM D638
Izod Impact, Notched  3.00 J/cm
@Thickness 3.20 mm,
Temperature 0.000 °C
5.62 ft-lb/in
@Thickness 0.126 in,
Temperature 32.0 °F
ASTM D256
 5.00 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
9.37 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Dart Drop, Total Energy  2.00 J
@Temperature -20.0 °C
1.48 ft-lb
@Temperature -4.00 °F
ASTM D1709-85
 5.50 J
@Temperature 0.000 °C
4.06 ft-lb
@Temperature 32.0 °F
ASTM D1709-85
 6.00 J
@Temperature 23.0 °C
4.43 ft-lb
@Temperature 73.4 °F
ASTM D1709-85
Dart Drop Total Energy  20.0 J/cm
@Temperature -20.0 °C
0.0375 ft-lb/mil
@Temperature -4.00 °F
 55.0 J/cm
@Temperature 0.000 °C
0.103 ft-lb/mil
@Temperature 32.0 °F
 60.0 J/cm
@Temperature 23.0 °C
0.112 ft-lb/mil
@Temperature 73.4 °F
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 145 °C293 °FASTM D1525
Heat Distortion Temperature 85.0 °C185 °FASTM D648
 
Descriptive Properties
ColorMapal Color Catalogue No. 520002

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mapal Plastics Maplon CFA-HK Polypropylene Sheet
Mapal Plastics Maplon PAPER MATCH Polypropylene Sheet
Mapal Plastics Maplon Type 3G Polypropylene Sheet
Mapal Plastics Maplon Type D Polypropylene Sheet
Mapal Plastics Maplon Type K OPAQLON COO1 Polypropylene Sheet

PMAPAL05 / 83616

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.