MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Fainplast Compounds MRT 256/G Medical Rigid PVC, Injection Molding
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes: Beta and gamma resistant connectors

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.29 - 1.33 g/cc0.0466 - 0.0480 lb/in³ISO R 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 29.0 MPa4210 psiISO R 527
Tensile Strength, Yield 31.0 MPa4500 psiISO R 527
Elongation at Break 210 %210 %ISO R 527
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 51.0 - 53.0 °C124 - 127 °FISO R 306
 
Descriptive Properties
Properties according to Pharmacopoeia 4th editionNO

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Colorite Polymers 2019F Rigid PVC
GEHR Plastics PVC-U Polyvinylchloride
Inovyn 257RF Polyvinyl Chloride General Purpose - Rigid
BASF Vinidur® Compound DB 8316 white PVC, Unplasticized
Inovyn 260RF Polyvinyl Chloride General Purpose - Rigid

PFAIN669 / 80871

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.