MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Röhm ACRYLITE® 32 mm Resist High Impact Acrylic Quad-Skin Sheet  (discontinued **)
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Optical Sheet

Material Notes: 32 mm ACRYLITER Resist high impact acrylic quad-skin sheet is a highly heat-insulating and weather-resistant quadruple-skinned sheet made of impact-modified acrylic (polymethyl methacrylate, PMMA) polymer. It is used in industrial and commercial buildings, sports arenas as well as for private applications, wherever isolative glazing with exceptional impact resistance, hail resistance and toughness, with the added benefits of quick and easy installation, is needed. 32 mm ACRYLITER Resist high impact acrylic quad-skin sheet is suitable for sloped and vertical applications including the following:
  • Canopies
  • Carports
  • Clerestory Glazing
  • Interior Walls
  • Interior Partitions
  • Lighting Panels
  • Conservatories
  • Skylights
  • Barrel Vaults
  • Facades & Cladding
  • Greenhouses
  • Pool Enclosures
  • Patio Covers
  • Sunrooms
Advantages of 32 mm ACRYLITE® Resist high impact acrylic quad-skin sheet
  • UV-resistant supported by a 30 year non yellowing guarantee
  • Offers excellent protection against excessive amounts of UV radiation.
  • Insulative characteristics offering up to 70% energy savings and minimizes CO2 emissions.
  • Hail-resistant with a 10-year guarantee for withstanding hailstones with a kinetic energy of 1 joule.
  • Available with the Heatstop infrared-reflecting coating
  • Impact resistance during transportation, handling and installation.
  • Range of colors and solar tints including a Heatstop infrared-reflecting sheet.
  • ACRYLITE® can be recycled in an environmentally friendly manner.

Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm (Roehm) GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 32.0 microns1.26 mil
 
Thermal PropertiesMetricEnglishComments
CTE, linear 162 µm/m-°C90.0 µin/in-°F
Thermal Conductivity 0.0504 W/m-K0.350 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 70.0 °C158 °F
Smoke Density 0.0850.085ASTM D2843
Ignition Temperature 443 °C830 °FAutoignition; ASTM D1929
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 40 %40 %Heatstop Pearl
 64 %64 %Light White
 76 %76 %Clear
 
Descriptive Properties
Rate of BurnC2/CC2ASTM D635
R-value3.57 °F/BTU-hr-ft2

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Röhm Acrylite® 8N Acrylic Polymer
Röhm Acrylite Plus® zdf Impact Acrylic Polymer
Röhm Acrylite Plus® zk3HR Impact Acrylic Polymer
Röhm Acrylite Plus® zk4BR Impact Acrylic Polymer
Röhm Acrylite Plus® zk4HR Impact Acrylic Polymer

PEVONIL006 / 196212

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.