MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Corning 1.8 / 35 BLANC High Index glass
Categories: Ceramic; Glass; Optical

Material Notes: Application : Ophthalmic lenses : Single vision, progressive addition

Information provided by Corning Incorporated.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.65 g/cc0.132 lb/in³
 
Thermal PropertiesMetricEnglishComments
CTE, linear 9.10 µm/m-°C5.06 µin/in-°F
Softening Point 732 °C1350 °F
Annealing Point 617 °C1140 °F
Strain Point 732 °C1350 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index  1.79522
@Wavelength 656.3 nm
1.79522
@Wavelength 656.3 nm
Line: C; Hydrogen
 1.79628
@Wavelength 643.8 nm
1.79628
@Wavelength 643.8 nm
Line: C'; Cadmium
 1.8020
@Wavelength 587.6 nm
1.8020
@Wavelength 587.6 nm
Line: d; Helium
 1.80749
@Wavelength 546.1 nm
1.80749
@Wavelength 546.1 nm
Line: e; Mercury
 1.81838
@Wavelength 486.1 nm
1.81838
@Wavelength 486.1 nm
Line: F; Hydrogen
 1.81978
@Wavelength 480 nm
1.81978
@Wavelength 480 nm
Line: F'; Cadmium
Abbe Number 34.434.4ve
 34.634.6vd
Transmission, Visible  84 %
@Wavelength 380 - 500 nm,
Thickness 2.00 mm
84 %
@Wavelength 380 - 500 nm,
Thickness 0.0787 in
Blue light transmission factor
 84.9 %
@Wavelength 380 - 780 nm,
Thickness 2.00 mm
84.9 %
@Wavelength 380 - 780 nm,
Thickness 0.0787 in
Luminous; ISO 8980-3
UV Transmittance  <= 0.10 %
@Thickness 2.00 mm
<= 0.10 %
@Thickness 0.0787 in
Solar UV-B transmission factor
 28.5 %
@Thickness 2.00 mm
28.5 %
@Thickness 0.0787 in
Solar UV-A transmission factor
 <= 0.10 %
@Wavelength 280 - 315 nm,
Thickness 2.00 mm
<= 0.10 %
@Wavelength 280 - 315 nm,
Thickness 0.0787 in
 38.5 %
@Wavelength 315 - 380 nm,
Thickness 2.00 mm
38.5 %
@Wavelength 315 - 380 nm,
Thickness 0.0787 in
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borosilicate Glass
96% Silica Consolidated Reconstructed Glass
Accuratus MACOR Machinable Glass Ceramic
Astro Met Macor® Machinable Glass Ceramic
Corning 1.6 / 41 BLANC TC Medium index glass, Chemtemperable

CCORN907 / 233318

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.