MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

JIS SKS95M Oil-hardening Cold Work Tool Steel
Categories: Metal; Ferrous Metal; Tool Steel; Cold Work Steel; Oil-Hardening Steel

Material Notes: Even intricate sections may be hardened, with good dimensional stability during hardening.

Key Words: JIS G3311(88) SKS95M, SKS 95M, SKS-95M; Comparable to AISI O2 Tool Steel, UNS T31502
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.61 g/cc0.275 lb/in³(AISI O2)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 200 - 290200 - 290
 
Thermal PropertiesMetricEnglishComments
CTE, linear  10.3 µm/m-°C
@Temperature 25.0 - 40.0 °C
5.72 µin/in-°F
@Temperature 77.0 - 104 °F
(AISI O2)
 13.0 µm/m-°C
@Temperature 25.0 - 260 °C
7.22 µin/in-°F
@Temperature 77.0 - 500 °F
(AISI O2)
 14.6 µm/m-°C
@Temperature 25.0 - 540 °C
8.11 µin/in-°F
@Temperature 77.0 - 1000 °F
(AISI O2)
 
Processing PropertiesMetricEnglishComments
Processing Temperature 175 - 260 °C347 - 500 °FTempering Temperature (AISI O2)
 760 - 800 °C1400 - 1470 °FHardening Temperature (AISI O2)
Annealing Temperature 745 - 775 °C1370 - 1430 °F(AISI O2)
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.80 - 0.90 %0.80 - 0.90 %
Chromium, Cr 0.20 - 0.60 %0.20 - 0.60 %
Copper, Cu <= 0.25 %<= 0.25 %
Iron, Fe 97.4 - 98.2 %97.4 - 98.2 %As Balance
Manganese, Mn 0.80 - 1.1 %0.80 - 1.1 %
Nickel, Ni <= 0.25 %<= 0.25 %
Phosphorus, P <= 0.030 %<= 0.030 %
Silicon, Si <= 0.50 %<= 0.50 %
Sulfur, S <= 0.030 %<= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type O2 Oil-hardening Tool Steel, oil quenched at 800°C, tempered at 260°C
Carpenter Stentor® Alloy Tool Steel (Oil-Hard) (AISI 02)
AISI Type A2 Tool Steel
Carpenter S7 Alloy Tool Steel (AISI S7)
Overview of materials for Oil-Hardening Steel

MSTJZSKS95M / 231089

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.