MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

TIMET TIMETAL® EXHAUST XT™ Low Alloyed Titanium
Categories: Metal; Nonferrous Metal; Titanium Alloy; Unalloyed/Modified Titanium

Material Notes: TIMETAL® EXHAUST XT™ is a low-alloy content titanium alloy suited for automotive and motorcycle exhausts and other industrial applications. Substantial weight savings are possible by substitution for stainless steel. It has superior oxidation resistance and elevated temperature strength compared to other commercially pure titanium alloys.

Data provided by TIMET.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.51 g/cc0.163 lb/in³Typical
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate >= 414 MPa>= 60000 psiAnnealed
 581 MPa84300 psiSheet
 80.0 MPa
@Temperature 775 °C
11600 psi
@Temperature 1430 °F
 150 MPa
@Temperature 650 °C
21800 psi
@Temperature 1200 °F
 300 MPa
@Temperature 425 °C
43500 psi
@Temperature 797 °F
Tensile Strength, Yield  >= 345 MPa
@Strain 0.2 %
>= 50000 psi
@Strain 0.2 %
Annealed
 531 MPa
@Strain 0.2 %
77000 psi
@Strain 0.2 %
Sheet
 80.0 MPa
@Strain 0.2 %,
Temperature 775 °C
11600 psi
@Strain 0.2 %,
Temperature 1430 °F
 125 MPa
@Strain 0.2 %,
Temperature 650 °C
18100 psi
@Strain 0.2 %,
Temperature 1200 °F
 275 MPa
@Strain 0.2 %,
Temperature 425 °C
39900 psi
@Strain 0.2 %,
Temperature 797 °F
Elongation at Break >= 20 %>= 20 %Annealed
 30 %30 %Sheet
 30 %
@Temperature 425 °C
30 %
@Temperature 797 °F
 68 %
@Temperature 650 °C
68 %
@Temperature 1200 °F
 85 %
@Temperature 775 °C
85 %
@Temperature 1430 °F
Creep Strength  69.0 MPa
@Temperature 427 °C,
Time 180000 sec
10000 psi
@Temperature 801 °F,
Time 50.0 hour
Creep Rate = 0.028%
 138 MPa
@Temperature 427 °C,
Time 180000 sec
20000 psi
@Temperature 801 °F,
Time 50.0 hour
Creep Rate = 0.108%
Bend Radius, Minimum <= 2.0 t<= 2.0 tSheet
 4.0 t4.0 tAnnealed
 
Thermal PropertiesMetricEnglishComments
CTE, linear  9.60 µm/m-°C
@Temperature 25.0 - 100 °C
5.33 µin/in-°F
@Temperature 77.0 - 212 °F
 10.0 µm/m-°C
@Temperature 25.0 - 800 °C
5.56 µin/in-°F
@Temperature 77.0 - 1470 °F
 10.4 µm/m-°C
@Temperature 25.0 - 500 °C
5.78 µin/in-°F
@Temperature 77.0 - 932 °F
Specific Heat Capacity 0.534 J/g-°C0.128 BTU/lb-°F
Thermal Conductivity 15.90 W/m-K110.3 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 425 °C797 °FContinuous
 540 °C1000 °FIntermittent
Beta Transus 920 °C1690 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.080 %<= 0.080 %
Hydrogen, H <= 0.015 %<= 0.015 %
Iron, Fe <= 0.30 %<= 0.30 %
Nitrogen, N <= 0.050 %<= 0.050 %
Other, each 0.10 %0.10 %
Other, total 0.40 %0.40 %
Oxygen, O <= 0.35 %<= 0.35 %
Silicon, Si 0.15 - 0.60 %0.15 - 0.60 %Nominal 0.45%
Titanium, Ti 99.5 %99.5 %As Remainder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arcam Ti6Al4V Titanium Alloy
TIMET TIMETAL® 6-4 ELI Titanium Alloy (Ti-6Al-4V ELI; ASTM Grade 23) (Annealed; <1.75 in Rod or Thickness; Per ASTM F136)
TIMET TIMETAL® 6-4 ELI Titanium Alloy (Ti-6Al-4V ELI; ASTM Grade 23) (Annealed; <3.0 in Rod or Thickness; Per ASTM B348)
Titanium Beta-21S (Grade 21)
American Elements Nickel Titanium Nanoparticles

NTIMEXT / 199546

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.