MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Molybdenum Alloy
Categories: Metal; Nonferrous Metal; Molybdenum Alloy

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Molybdenum Alloy". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Eagle Alloys Corporation is a leading supplier of quality metals and alloys. Our staff prides itself on working fast, efficiently and courteously to get you the information you need. Call (800) 237-9012 or visit www.EagleAlloys.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.52 - 14.6 g/cc0.0549 - 0.527 lb/in³Average value: 10.1 g/cc Grade Count:101
Particle Size 0.0300 - 90.0 µm0.0300 - 90.0 µmAverage value: 35.7 µm Grade Count:13
 
Chemical PropertiesMetricEnglishComments
Thermal Neutron Cross Section 2.50 barns/atom2.50 barns/atomAverage value: 2.50 barns/atom Grade Count:3
Electrode Potential -0.200 V-0.200 VAverage value: -0.200 V Grade Count:3
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 120 - 225120 - 225Average value: 181 Grade Count:8
Hardness, Rockwell A 58.0 - 60.058.0 - 60.0Average value: 58.7 Grade Count:3
Hardness, Rockwell B 67.0 - 98.067.0 - 98.0Average value: 81.9 Grade Count:13
Hardness, Vickers 155 - 320155 - 320Average value: 243 Grade Count:21
Tensile Strength, Ultimate 280 - 3900 MPa40600 - 566000 psiAverage value: 693 MPa Grade Count:46
Tensile Strength, Yield 241 - 860 MPa35000 - 125000 psiAverage value: 569 MPa Grade Count:34
Elongation at Break 1.00 - 40.0 %1.00 - 40.0 %Average value: 11.1 % Grade Count:35
Modulus of Elasticity 200 - 365 GPa29000 - 52900 ksiAverage value: 306 GPa Grade Count:31
Compressive Yield Strength 400 MPa58000 psiAverage value: 400 MPa Grade Count:3
Bulk Modulus 272 GPa39500 ksiAverage value: 272 GPa Grade Count:3
Poissons Ratio 0.285 - 0.3800.285 - 0.380Average value: 0.332 Grade Count:6
Shear Modulus 120 - 132 GPa17400 - 19100 ksiAverage value: 126 GPa Grade Count:6
Shear Strength 500 MPa72500 psiAverage value: 500 MPa Grade Count:3
Bend Radius, Minimum 1.00 - 2.00 t1.00 - 2.00 tAverage value: 1.67 t Grade Count:3
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000370 - 0.0000220 ohm-cm0.00000370 - 0.0000220 ohm-cmAverage value: 0.00000707 ohm-cm Grade Count:35
Magnetic Susceptibility 9.30e-79.30e-7Average value: 9.30e-7 Grade Count:3
 
Thermal PropertiesMetricEnglishComments
CTE, linear 4.30 - 10.7 µm/m-°C2.39 - 5.94 µin/in-°FAverage value: 6.33 µm/m-°C Grade Count:40
Specific Heat Capacity 0.217 - 0.305 J/g-°C0.0519 - 0.0729 BTU/lb-°FAverage value: 0.255 J/g-°C Grade Count:21
Thermal Conductivity 36.8 - 310 W/m-K255 - 2150 BTU-in/hr-ft²-°FAverage value: 172 W/m-K Grade Count:52
Melting Point 980 - 2620 °C1800 - 4750 °FAverage value: 2340 °C Grade Count:32
Solidus 980 - 2500 °C1800 - 4530 °FAverage value: 1140 °C Grade Count:11
Liquidus 2600 - 2620 °C4710 - 4750 °FAverage value: 2610 °C Grade Count:17
Boiling Point 4610 - 4800 °C8330 - 8670 °FAverage value: 4650 °C Grade Count:13
Maximum Service Temperature, Air 400 - 2000 °C752 - 3630 °FAverage value: 1090 °C Grade Count:16
 
Optical PropertiesMetricEnglishComments
Reflection Coefficient, Visible (0-1) 0.4600.460Average value: 0.460 Grade Count:3
 
Processing PropertiesMetricEnglishComments
Recrystallization Temperature 1100 - 2000 °C2010 - 3630 °FAverage value: 1310 °C Grade Count:11
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.00100 - 0.0100 %0.00100 - 0.0100 %Average value: 0.00260 % Grade Count:28
Antimony, Sb 0.0400 - 0.0800 %0.0400 - 0.0800 %Average value: 0.0567 % Grade Count:6
Arsenic, As 0.000500 - 0.220 %0.000500 - 0.220 %Average value: 0.0623 % Grade Count:14
Bismuth, Bi 0.0500 - 0.150 %0.0500 - 0.150 %Average value: 0.0900 % Grade Count:4
Cadmium, Cd 0.000500 - 0.00150 %0.000500 - 0.00150 %Average value: 0.00123 % Grade Count:15
Calcium, Ca 0.00100 - 0.0100 %0.00100 - 0.0100 %Average value: 0.00264 % Grade Count:24
CaO 1.50 - 3.00 %1.50 - 3.00 %Average value: 2.22 % Grade Count:10
Carbon, C 0.00100 - 6.10 %0.00100 - 6.10 %Average value: 0.235 % Grade Count:81
Chromium, Cr 0.000500 - 4.00 %0.000500 - 4.00 %Average value: 0.192 % Grade Count:41
Cobalt, Co 0.00100 - 0.00300 %0.00100 - 0.00300 %Average value: 0.00175 % Grade Count:6
Copper, Cu 0.00100 - 50.0 %0.00100 - 50.0 %Average value: 6.25 % Grade Count:61
Hafnium, Hf 0.800 - 1.40 %0.800 - 1.40 %Average value: 1.06 % Grade Count:5
Hydrogen, H 0.000500 - 0.00100 %0.000500 - 0.00100 %Average value: 0.000688 % Grade Count:8
Iron, Fe 0.00200 - 43.2 %0.00200 - 43.2 %Average value: 4.02 % Grade Count:77
Lanthanum, La 0.150 - 1.20 %0.150 - 1.20 %Average value: 0.718 % Grade Count:6
Lead, Pb 0.000500 - 0.650 %0.000500 - 0.650 %Average value: 0.0847 % Grade Count:36
Magnesium, Mg 0.00100 - 0.0100 %0.00100 - 0.0100 %Average value: 0.00134 % Grade Count:28
Manganese, Mn 0.000200 - 0.00500 %0.000200 - 0.00500 %Average value: 0.00109 % Grade Count:16
Mercury, Hg 0.000100 %0.000100 %Average value: 0.000100 % Grade Count:3
Molybdenum, Mo 45.0 - 100 %45.0 - 100 %Average value: 86.1 % Grade Count:161
Nickel, Ni 0.00100 - 17.2 %0.00100 - 17.2 %Average value: 0.526 % Grade Count:64
Niobium, Nb (Columbium, Cb) 0.00100 - 9.70 %0.00100 - 9.70 %Average value: 3.23 % Grade Count:3
Nitrogen, N 0.00100 - 0.00500 %0.00100 - 0.00500 %Average value: 0.00188 % Grade Count:41
O2 0.150 - 9.50 %0.150 - 9.50 %Average value: 2.33 % Grade Count:4
Oxygen, O 0.00150 - 4.00 %0.00150 - 4.00 %Average value: 0.133 % Grade Count:58
Phosphorus, P 0.00200 - 0.100 %0.00200 - 0.100 %Average value: 0.0445 % Grade Count:21
Potassium, K 0.00200 - 42.3 %0.00200 - 42.3 %Average value: 12.0 % Grade Count:33
Rhenium, Re 5.00 - 47.5 %5.00 - 47.5 %Average value: 35.9 % Grade Count:6
Silicon, Si 0.00200 - 2.58 %0.00200 - 2.58 %Average value: 0.234 % Grade Count:75
Silver, Ag 0.000500 - 50.0 %0.000500 - 50.0 %Average value: 26.7 % Grade Count:12
SiO2 5.00 - 13.0 %5.00 - 13.0 %Average value: 8.05 % Grade Count:10
Sodium, Na 0.00100 - 2.60 %0.00100 - 2.60 %Average value: 0.164 % Grade Count:16
Sulfur, S 0.00200 - 0.200 %0.00200 - 0.200 %Average value: 0.100 % Grade Count:11
Tantalum, Ta 0.00200 - 11.0 %0.00200 - 11.0 %Average value: 5.45 % Grade Count:4
Tin, Sn 0.000500 - 0.0800 %0.000500 - 0.0800 %Average value: 0.0199 % Grade Count:44
Titanium, Ti 0.00100 - 20.0 %0.00100 - 20.0 %Average value: 1.17 % Grade Count:34
Tungsten, W 0.0300 - 50.0 %0.0300 - 50.0 %Average value: 9.55 % Grade Count:31
Zinc, Zn 0.000500 - 0.00100 %0.000500 - 0.00100 %Average value: 0.000800 % Grade Count:5
Zirconium, Zr 0.000500 - 0.300 %0.000500 - 0.300 %Average value: 0.0910 % Grade Count:20

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Stainless Steel
Overview of materials for Refractory Metal
Overview of materials for Nickel Alloy
Overview of materials for Tungsten Alloy
Overview of materials for T 400 Series Stainless Steel

M01060 / 81673

Metalmen Sales

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.