MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Low brass 80%, UNS C24000, OS050 Temper, Flat Products & Wire
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Temper: Nominal Grain Size 0.050 mm

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Capacity for Being Cold Worked; Good Suitability – Oxyacetylene Welding, Gas Shielded Arc Welding, Butt Weld; Fair Suitability – Spot Weld, Capacity for Being Hot Formed

Common Fabrication Processes: Blanking; Drawing; Etching; Forming and Bending; Heading and Upsetting; Piercing and Punching; Roll Threading and Knurling; Shearing; Spinning; Squeezing and Swaging; Stamping

Typical uses: Medallions; Ornamental Components; Spandrels; Decorative Panels; Clock Dials; Musical Instrument Parts; Plaques; Battery Caps; Rotor Bars, AC Motors; Flexible Hose; Flexible Hose Bellows; Pump Lines; Welding Wire; Tokens

Applicable Specifications: Bar – ASTM B36/B36M, ASTM B19; Brazing Filler Metal – FEDERAL QQ-B-650; Cups – ASTM B19; Plate - ASTM B36/B36M, ASTM B19; Rod, Bar & Shapes - ASTM B927/B927M; Sheet - SAE J463; ASTM B36/B36M, SAE J461; Strip - SAE J461, ASTM B36/B36M, SAE J463; Strip, Sheet & Plate – ASTM B19; Wire – ASTM B134/B134M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.66 g/cc0.313 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength  303 MPa
@Thickness 2.03 mm
44000 psi
@Thickness 0.0800 in
 303 MPa
@Thickness 1.02 mm
44000 psi
@Thickness 0.0400 in
Tensile Strength, Yield 96.5 MPa
@Thickness 1.02 mm
14000 psi
@Thickness 0.0400 in
0.5% Ext
Elongation at Break  50 %
@Thickness 1.02 mm
50 %
@Thickness 0.0400 in
 55 %
@Thickness 2.03 mm
55 %
@Thickness 0.0800 in
Tensile Modulus 110 GPa16000 ksi
Modulus of Rigidity 41.4 GPa6000 ksi
Poissons Ratio 0.330.33Calculated
Machinability 30 %30 %
Shear Strength  221 MPa
@Thickness 2.03 mm
32000 psi
@Thickness 0.0800 in
 221 MPa
@Thickness 1.02 mm
32000 psi
@Thickness 0.0400 in
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000540 ohm-cm0.00000540 ohm-cm32% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 19.1 µm/m-°C
@Temperature 20.0 - 300 °C
10.6 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.377 J/g-°C0.0900 BTU/lb-°F
Thermal Conductivity 11.7 W/m-K81.0 BTU-in/hr-ft²-°F
Melting Point 966 - 999 °C1770 - 1830 °F
Solidus 966 °C1770 °F
Liquidus 999 °C1830 °F
Annealing Point 427 - 704 °C800 - 1300 °F
 
Processing PropertiesMetricEnglishComments
Hot-Working Temperature 816 - 899 °C1500 - 1650 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 78.5 - 81.5 %78.5 - 81.5 %
Iron, Fe <= 0.050 %<= 0.050 %
Lead, Pb <= 0.050 %<= 0.050 %
Zinc, Zn 18.5 - 21.5 %18.5 - 21.5 %As Balance
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC24000x3 / 292899

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.