MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco AREMCOLOX™ 502-600 Machinable Glass Ceramic
Categories: Ceramic; Glass; Glass Ceramic; Machinable Ceramic

Material Notes: Recommended for high dielectric and mechanical strength requirements and temperatures to 1100 ºF (593 ºC). Used for high voltage insulators, lamp housings, insulation sleeves and washers, thermal switches, and radiation parts. Readily machined and no firing required. Plates are available from ?” to 1” thick; rods from ¼” to 1” diameter.

Vendors: Aremco offers a range of machinable ceramics. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.80 g/cc2.80 g/cc
Water Absorption 0.00 %0.00 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell A 4747
Flexural Strength 75.8 MPa11000 psi
Compressive Strength 221 MPa32000 psi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cm
Dielectric Constant 6.8
@Frequency 1e+6 Hz
6.8
@Frequency 1e+6 Hz
Dielectric Strength 15.0 kV/mm380 kV/in
Dissipation Factor 0.012
@Frequency 1e+6 Hz
0.012
@Frequency 1e+6 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 10.4 µm/m-°C
@Temperature 20.0 °C
5.80 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 1.30 W/m-K9.02 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 593 °C1100 °FOxidizing
Maximum Service Temperature, Inert 593 °C1100 °F
 593 °C1100 °FVacuum

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aremco AREMCOLOX™ 502-400 Machinable Glass Ceramic
Aremco AREMCOLOX™ 502-800 Macor® Machinable Glass Ceramic, MGC
Advanced Ceramics ACL 2089 Cordierite
96% Silica Consolidated Reconstructed Glass
Aremco AREMCOLOX™ 502-1550 (Med. Density) Machinable Zirconium Phosphate

CAREM01 / 542

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.