MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik VESTAMID® CW1442 BK Nylon 12, Carbon Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, Carbon Fiber Filled

Material Notes: VESTAMID® CW1442 BK is a highly filled, carbon fiber-reinforced, heat- and UV-stabilized compound based on PA12. It is generally used for components manufactured in the injection molding process and is especially suitable for applications where high impact strength and stiffness as well as low coefficient of friction are required. In addition, it has a good bonding strength with TPU. The PA12 compound absorbs only small amounts of water. Therefore, components made from this material have an excellent dimensional accuracy with changing ambient humidity. Due to the low melting point of VESTAMID® CW1442 BK, the material provides a wide processing window for the injection molding process. The compound is suitable for applications requiring a high ratio of flow length to wall thickness. Preliminary data sheet. VESTAMID® CW1442 BK is supplied as cylindrical granules ready for processing, in moisture barrier bags. The use of colorants can change property values.
Dry properties listed below
Industrial Sector: Sports and Lifestyle
Processing: Injection molding
Delivery form: Pellets, Granules
Resistance to: Heat (thermal stability), UV / light / weathering
Electrical: Insulating
Additives: Carbon fibers
Applications: General purpose
Processing: Thermoforming
Special Characteristics: U.V. stabilized
Color: Black
Additives: Heat stabilizer
Delivery form: Cylindrical pellets
Chemical Resistance: General chemical resistance

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³ISO 1183
Water Absorption 0.200 %0.200 %Sim to ISO 62
Moisture Absorption 0.0700 %0.0700 %Sim to ISO 62
Linear Mold Shrinkage, Flow 0.000 cm/cm0.000 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.00200 cm/cm0.00200 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 80.080.0ISO 7619-1
Tensile Strength at Break 137 MPa19900 psiISO 527
Tensile Strength 137 MPa19900 psiISO 527
Elongation at Break 5.00 %5.00 %Nominal; ISO 527
 5.00 %5.00 %ISO 527
Tensile Modulus 12.6 GPa1830 ksiISO 527
Flexural Strength 109 MPa15800 psiat break; ISO 178
 196 MPa28400 psiat conv. Deflection; ISO 178
 201 MPa29200 psiISO 178
Flexural Modulus 12.0 GPa1740 ksiISO 178
Flexural Strain at Break 4.00 %4.00 %at flexural strength; ISO 178
 5.00 %5.00 %ISO 178
Charpy Impact Unnotched  7.90 J/cm²
@Temperature -30.0 °C
37.6 ft-lb/in²
@Temperature -22.0 °F
Type of failure: C; ISO 179/1eU
 8.30 J/cm²
@Temperature 23.0 °C
39.5 ft-lb/in²
@Temperature 73.4 °F
Type of failure: C; ISO 179/1eU
Charpy Impact, Notched  1.60 J/cm²
@Temperature -30.0 °C
7.61 ft-lb/in²
@Temperature -22.0 °F
Type of failure: C; ISO 179/1eA
 2.40 J/cm²
@Temperature 23.0 °C
11.4 ft-lb/in²
@Temperature 73.4 °F
Type of failure: P; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 176 °C349 °FISO 11357-1/-3
 
Processing PropertiesMetricEnglishComments
Melt Temperature 270 °C518 °F
Mold Temperature 60.0 °C140 °F
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIK7881 / 325013

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.