MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aluminum 2011-T4
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 2000 Series Aluminum Alloy

Key Words: UNS A92011; AA2011-T3; Al2011-T3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.82 g/cc0.102 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate >= 275 MPa
@Thickness 9.52 - 203 mm,
Temperature 20.0 °C
>= 39900 psi
@Thickness 0.375 - 8.00 in,
Temperature 68.0 °F
Rolled or cold finished wire, rod, and bar
Tensile Strength, Yield >= 125 MPa
@Thickness 9.52 - 203 mm
>= 18100 psi
@Thickness 0.375 - 8.00 in
Rolled or cold finished wire, rod, and bar
Elongation at Break >= 16 %
@Thickness 9.52 - 203 mm
>= 16 %
@Thickness 0.375 - 8.00 in
Rolled or cold finished wire, rod, and bar
Modulus of Elasticity 70.0 GPa10200 ksi
Poissons Ratio <= 0.33<= 0.33
Shear Modulus 26.0 GPa3770 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000440 ohm-cm0.00000440 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  21.4 µm/m-°C
@Temperature -50.0 - 20.0 °C
11.9 µin/in-°F
@Temperature -58.0 - 68.0 °F
 23.1 µm/m-°C
@Temperature 20.0 - 100 °C
12.8 µin/in-°F
@Temperature 68.0 - 212 °F
 24.0 µm/m-°C
@Temperature 20.0 - 200 °C
13.3 µin/in-°F
@Temperature 68.0 - 392 °F
 25.0 µm/m-°C
@Temperature 20.0 - 300 °C
13.9 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.864 J/g-°C0.207 BTU/lb-°F
Thermal Conductivity 152 W/m-K1050 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 91.85 - 94.8 %91.85 - 94.8 %
Copper, Cu 5.0 - 6.0 %5.0 - 6.0 %
Iron, Fe <= 0.70 %<= 0.70 %
Lead, Pb 0.20 - 0.60 %0.20 - 0.60 %
Other, each <= 0.050 %<= 0.050 %
Other, total <= 0.15 %<= 0.15 %
Silicon, Si <= 0.40 %<= 0.40 %
Zinc, Zn <= 0.30 %<= 0.30 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 2011-T6
Aluminum 2011-T3
Aluminum 2011-T8
Aluminum 2007-T3
Aluminum Alloys, General

MA2011T4 / 109162

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.