Description Polytrope TPP 403 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains special heat stabilizers to allow usage in the under-hood environment. TPP 402 is only available in black compounds and is not UV stable.