MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Arlon Electronic Materials 37N Polyimide Low-Flow
Categories: Polymer; Thermoset; Polyimide, TS

Material Notes: 37N is a polyimide low-flow prepreg suitable for bonding multilayer polyimide rigid-flex, attaching heat sinks to polyimide MLBs, or other applications where minimal and uniform resin flow is required.

  • Tg > 200°C and expansion characteristics typical of polyimide greatly improves PTH reliability
  • Good bond strength to Kapton® polyimide, copper and other metals
  • Curable at temperatures as low as 350°F
  • Excellent thermal stability
  • Available in different flow ranges and fiberglass styles for optimal process flexibility
  • Electrical and mechanical properties meeting the requirements of IPC-4101/42
  • Compatible with lead-free solder processing
  • RoHS/WEEE compliant

Typical Applications:

  • Bonding multilayer polyimide rigid-flex
  • Attaching heat sinks to polyimide MLBs
  • Other applications where minimal and uniform resin flow is required

    Information provided by ARLON Electronic Materials.

  • Vendors: Arlon Materials for Electronics (MED) is a major manufacturer of specialty high performance laminate and prepreg materials for use in a wide variety of printed circuit board (PCB) applications and in several distinctive markets.

    Click here to view all available suppliers for this material.

    Please click here if you are a supplier and would like information on how to add your listing to this material.

     
    Physical PropertiesMetricEnglishComments
    Water Absorption <= 1.0 %<= 1.0 %IPC TM-650 2.6.2.1
     
    Mechanical PropertiesMetricEnglishComments
    Tensile Strength 221 MPa32000 psiIPC TM-650 2.4.18.3
    Flexural Strength 414 MPa60000 psiIPC TM-650 2.4.4
    Poissons Ratio 0.170.17ASTM D3039
    Peel Strength 0.736 kN/m4.20 pliTo Kapton, as received
     0.964 kN/m5.50 pliTo Copper (1 oz./35 micron); At Elevated Temperatures; IPC TM-650 2.4.8.2
     1.19 kN/m6.80 pliTo Copper (1 oz./35 micron); After Thermal Stress; IPC TM-650 2.4.8
     1.61 kN/m9.20 pliTo Copper (1 oz./35 micron); After Process Solutions; IPC TM-650 2.4.8
     
    Electrical PropertiesMetricEnglishComments
    Volume Resistivity 4.70e+15 ohm-cm4.70e+15 ohm-cmE24/125; IPC TM-650 2.5.17.1
     8.20e+15 ohm-cm8.20e+15 ohm-cmC96/35/90; IPC TM-650 2.5.17.1
    Surface Resistance 4.40e+12 ohm4.40e+12 ohmC96/35/90; IPC TM-650 2.5.17.1
     1.20e+15 ohm1.20e+15 ohmE24/125; IPC TM-650 2.5.17.1
    Dielectric Constant 4.25
    @Frequency 1e+6 Hz
    4.25
    @Frequency 1e+6 Hz
    may vary with resin %; IPC TM-650 2.5.5.3
    Dielectric Strength 52.4 kV/mm1330 kV/inIPC TM-650 2.5.6.2
    Dissipation Factor 0.018
    @Frequency 1e+6 Hz
    0.018
    @Frequency 1e+6 Hz
    IPC TM-650 2.5.5.3
    Arc Resistance 124 sec124 secIPC TM-650 2.5.1
     
    Thermal PropertiesMetricEnglishComments
    CTE, linear 16.0 µm/m-°C8.89 µin/in-°F
    CTE, linear, Transverse to Flow 76.0 µm/m-°C42.2 µin/in-°Fz, below Tg; IPC TM-650 2.4.24
     252 µm/m-°C140 µin/in-°Fz, above Tg; IPC TM-650 2.4.24
    Thermal Conductivity 0.300 W/m-K2.08 BTU-in/hr-ft²-°FASTM E1461
    Glass Transition Temp, Tg 210 °C410 °FTMA; IPC TM-650 2.4.24
    Decomposition Temperature 322 °C612 °FOnset; IPC TM-650 2.3.41
     340 °C644 °F5 percent; IPC TM-650 2.3.41
    Flammability, UL94 V-0V-0
     
    Descriptive Properties
    IPC Delamination - T260 (minutes)> 60IPC TM-650 2.4.24.1
    IPC Delamination - T288 (minutes)5IPC TM-650 2.4.24.1
    IPC Delamination - T300 (minutes)2IPC TM-650 2.4.24.1
    Z-Axis Expansion (%)2.3IPC TM-650 2.4.24 (50-260°C)

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Rogers Arlon AD1000 PTFE/Woven Fiberglass/Ceramic Filled Laminate for Microwave Printed Circuit Boards
    Rogers Arlon CLTE Microwave Printed Circuit Board Substrate
    Arlon Electronic Materials 85N Polyimide Laminate and Prepreg
    Arlon Electronic Materials EP2 Enhanced Polyimide Laminate and Prepreg
    Arlon Electronic Materials 35N Fast Cure Polyimide Laminate and Prepreg

    PARLM9876 / 149029

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.