MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Mocom (ALBIS) ALCOM® PC 740/1.1 CF20 PC, 20% Carbon Fiber Reinforced
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Carbon Fiber Reinforced

Material Notes: Base Polymer: Polycarbonate

Filler/Additive System: 20% Carbon Fiber

Special Features: Electrically conductive, reduced surface resistivity, high stiffness, heat ageing stabilization

Market Segment: Machinery, various

Application Area: Injection molded parts

Typical Applications: Functional components, housings, protection cap

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.28 g/cc0.0462 lb/in³ISO 1183
Maximum Moisture Content 0.0200.020
Linear Mold Shrinkage, Flow 0.0010 - 0.0020 cm/cm
@Time 86400 sec
0.0010 - 0.0020 in/in
@Time 24.0 hour
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0010 - 0.0030 cm/cm
@Time 86400 sec
0.0010 - 0.0030 in/in
@Time 24.0 hour
ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 160 MPa23200 psiISO 527
Elongation at Break 2.1 %2.1 %ISO 527
Tensile Modulus 13.8 GPa2000 ksiISO 527
Flexural Strength 230 MPa33400 psiISO 178
Flexural Modulus 12.8 GPa1860 ksiISO 178
Charpy Impact Unnotched 4.30 J/cm²20.5 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.850 J/cm²4.04 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Surface Resistance <= 200 ohm<= 200 ohmIEC 62631-3-2
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 143 °C289 °FISO 75-1/-2
Vicat Softening Point 150 °C302 °FB50; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 310 - 330 °C590 - 626 °FInjection molding
Mold Temperature 80.0 - 130 °C176 - 266 °FInjection molding
Drying Temperature  100 - 120 °C
@Time 14400 - 43200 sec
212 - 248 °F
@Time 4.00 - 12.0 hour
in air circulating dryer
 120 °C
@Time 7200 - 10800 sec
248 °F
@Time 2.00 - 3.00 hour
in a dry air (desiccant) dryer
 
Descriptive Properties
Base PolymerPolycarbonate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® UHM Carbon Fiber (3000 Filaments)
Hexcel® UHM Carbon Fiber (12,000 Filaments)
S-Glass Fiber, Generic
LATI Larpeek 10 K/30 PEEK, 30% Carbon Fiber Reinforced
CoorsTek PlasmaPure-UC™ 99.9% Alumina

PALBIS8123 / 242182

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.