MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC CYCOLAC™ HMG47MD ABS (Americas)
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: General purpose, injection molding ABS for medical applications. Biocompatible (ISO 10993). FDA compliant. Gamma & EtO sterilizable.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/ccASTM D792
Density 1.05 g/cc0.0379 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0050 - 0.0080 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0080 in/in
@Thickness 0.126 in
SABIC method
Melt Flow  5.6 g/10 min
@Load 3.80 kg,
Temperature 230 °C
5.6 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
 19 g/10 min
@Load 10.0 kg,
Temperature 220 °C
19 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 33.0 MPa4790 psi5 mm/min; ASTM D638
 35.0 MPa5080 psi5 mm/min; ISO 527
Tensile Strength, Yield 44.0 MPa6380 psi5 mm/min; ASTM D638
 50.0 MPa7250 psi5 mm/min; ISO 527
Elongation at Break 24 %24 %5 mm/min; ASTM D638
 24.8 %24.8 %5 mm/min; ISO 527
Elongation at Yield 2.0 %2.0 %5 mm/min; ASTM D638
 2.6 %2.6 %5 mm/min; ISO 527
Tensile Modulus 2.27 GPa329 ksi5 mm/min; ASTM D638
 2.53 GPa367 ksi1mm/min; ISO 527
Flexural Yield Strength 72.0 MPa10400 psi1.3 mm/min, 50 mm span; ASTM D790
 76.0 MPa11000 psi2 mm/min; ISO 178
Flexural Modulus 2.34 GPa339 ksi1.3 mm/min, 50 mm span; ASTM D790
 2.41 GPa350 ksi2 mm/min; ISO 178
Izod Impact, Notched 3.20 J/cm5.99 ft-lb/inASTM D256
 1.33 J/cm
@Temperature -30.0 °C
2.49 ft-lb/in
@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 23.0 kJ/m²10.9 ft-lb/in²80*10*4; ISO 180/1A
 8.00 kJ/m²
@Temperature -30.0 °C
3.81 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Dart Drop, Total Energy 30.0 J22.1 ft-lbASTM D3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 88.2 µm/m-°C
@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 88.2 µm/m-°C
@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C
@Thickness 3.20 mm
201 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C176 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 80.0 °C
@Thickness 3.20 mm
176 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 98.0 °C208 °FRate B/50; ASTM D1525
 100 °C212 °FRate B/50; ISO 306
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 220 - 260 °C428 - 500 °FInjection Molding
Zone 1 190 - 210 °C374 - 410 °F
Zone 2 205 - 225 °C401 - 437 °F
Zone 3 215 - 240 °C419 - 464 °F
Melt Temperature 220 - 260 °C428 - 500 °F
Mold Temperature 50.0 - 70.0 °C122 - 158 °F
Drying Temperature 80.0 - 95.0 °C176 - 203 °FInjection Molding
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection Molding
 8.00 hour8.00 hourCumulative; Injection Molding
Moisture Content 0.10 %0.10 %
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 50 - 70 %50 - 70 %
Vent Depth 0.00380 - 0.00510 cm0.00150 - 0.00201 in
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI10045 / 243512

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.