MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Gallium Nitride, GaN
Categories: Ceramic; Nitride; Other Engineering Material; Semiconductor

Key Words: Pnictide; Semiconductor
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 6.10 g/cc0.220 lb/in³
a Lattice Constant 3.19 Å3.19 Å
c Lattice Constant 5.189 Å5.189 Å
Molecular Weight 83.73 g/mol83.73 g/mol
 
Electrical PropertiesMetricEnglishComments
Band Gap 3.34 eV3.34 eV
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 65.6 W/m-K455 BTU-in/hr-ft²-°F
Melting Point 1227 °C2241 °F
Decomposition Temperature >= 600 °C>= 1110 °F
 
Descriptive Properties
CAS Number25617-97-4
ColorGray
Crystal StructureHexagonalWurtzite (Zincite) Structure - Space Group P 63mc

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Gallium Arsenide, GaAs
MarkeTech AN 180 Aluminum Nitride Ceramic Substrate, 99% Purity
Copper, Cu; Cold-Worked
Aluminum Nitride, AlN
Silicon Carbide, Alpha SiC

DSEM88 / 3002

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.