MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Bamberger Polymers Bapolene® 615FP LLDPE, Metallocene Film Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: This resin is a metallocene product designed for applications requiring a combination of superior impact and seal properties. It contains slip and antiblocking additives and a process aid. It complies with US FDA 21CRR177.1520.

Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.918 g/cc0.0332 lb/in³ASTM D1505
Thickness 25.4 microns1.00 mil2.5:1 blow-up ratio, as tested
Melt Flow 1.5 g/10 min
@Load 10.0 kg,
Temperature 220 °C
1.5 g/10 min
@Load 22.0 lb,
Temperature 428 °F
cm³/10min Volumetric; ISO 1133
Antiblock Level 4800 ppm4800 ppm
Slip Level 100 ppm100 ppm
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 500 %500 %ASTM D882
Film Elongation at Break, TD 580 %580 %ASTM D882
Elmendorf Tear Strength MD 240 g
@Thickness 0.0254 mm
240 g
@Thickness 0.00100 in
ASTM D1922
Elmendorf Tear Strength TD 450 g
@Thickness 0.0254 mm
450 g
@Thickness 0.00100 in
ASTM D1922
Elmendorf Tear Strength, MD 9.45 g/micron240 g/milASTM D1922
Elmendorf Tear Strength, TD 17.7 g/micron450 g/milASTM D1922
Dart Drop 17.3 g/micron440 g/milASTM D1709
Dart Drop Test 440 g
@Thickness 0.0254 mm
0.970 lb
@Thickness 0.00100 in
ASTM D1709
Film Tensile Strength at Break, MD 9.03 MPa1310 psiASTM D882
Film Tensile Strength at Break, TD 9.03 MPa1310 psiASTM D882
 
Compliance PropertiesMetricEnglishComments
FDA YesYesFDA 21CRR177.1520.
 
Descriptive Properties
Processing MethodFilm Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBP1226 / 291423

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.