System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Möller Medical NanoSkin 101 NanoCoating
(discontinued **)
Categories:
Ceramic
;
Glass
;
Glass Ceramic
;
Other Engineering Material
;
Ceramic/Metallic Coating
Material Notes:
Hard, scratch-resistant, brittle coating with resistance to high temperatures and chemicals, bioinert.
Information provided by Möller Medical, Member of CENTROTEC Group
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Thickness
1.00
-
3.00
microns
0.0394
-
0.118
mil
Mechanical Properties
Metric
English
Comments
Taber Abrasion, mg/1000 Cycles
40
40
CS17 friction disc with 500g load; DIN 53754
Thermal Properties
Metric
English
Comments
Maximum Service Temperature, Air
600
°C
1110
°F
Processing Properties
Metric
English
Comments
Processing Temperature
200
-
340
°C
392
-
644
°F
Hardening Temperature
Descriptive Properties
Applicable Substrate
Aluminum
Brass
Copper
Glass
Stainless Steel
Tubes int. dia. 0.1-10 mm
Biocompatibility
Biocompatible
One-parametric cytotoxicity test
Contact Angle to Water [deg]
101
Cupping Test [mm]
<0.5
DIN EN ISO 1520
Non-Applicable Substrate
ABS
Nylon
PMMA
Polycarbonate
Pendulum Dampening Test [sec]
240-260
DIN EN ISO 1522
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Celanese VECTRA MT1335 LCP, Medical Technology
Covestro Texin® 5250 Thermoplastic Polyurethane, Polyether-based, Medical
NuSil MED-166 Silicone, Primer - Unrestricted Medical Use
AgPd-4 Precious dental alloy
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Hot Worked
CMOLL08 / 1629
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.