MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

AISI 1050 Steel, cold drawn, high temperature, stress relieved, 22-32 mm (0.875-1.25 in) round
Categories: Metal; Ferrous Metal; Carbon Steel; AISI 1000 Series Steel; Medium Carbon Steel

Material Notes: The composition listed applies only to structural shapes, plates, strip, and welded tubing. Semifinished products for forging, hot-rolled and cold-finished bars, wire rods, and seamless tubing have a carbon range of 0.48 - 0.55%.

Key Words: UNS G10500, AMS 5085, ASTM A29, ASTM A510, ASTM A519, ASTM A576, ASTM A682, DIN 1.1210, JIS S 53 C, JIS S 55 C, FED QQ-S-635 (C1050), FED QQ-S-700 (C1050), MIL SPEC MIL-S-16974, SAE J403, SAE J412, SAE J414
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.87 g/cc0.284 lb/in³Typical for steels.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 179179
Hardness, Knoop 200200Converted from Brinell
Hardness, Rockwell B 8888Converted from Brinell
Hardness, Vickers 188188Converted from Brinell
Tensile Strength, Ultimate 620 MPa89900 psi
Tensile Strength, Yield 515 MPa74700 psi
Elongation at Break 15 %15 %in 50 mm
Reduction of Area 40 %40 %
Modulus of Elasticity 200 GPa29000 ksiTypical for steel
Bulk Modulus 160 GPa23200 ksiTypical for steel
Poissons Ratio 0.290.29Typical For Steel
Shear Modulus 80.0 GPa11600 ksiTypical for steels.
Izod Impact 18.0 J13.3 ft-lbannealed at 790°C (1450°F)
 27.0 J19.9 ft-lbnormalized at 900°C (1650°F)
 31.0 J22.9 ft-lbas rolled
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  0.0000163 ohm-cm
@Temperature 0.000 °C
0.0000163 ohm-cm
@Temperature 32.0 °F
annealed specimen
 0.0000224 ohm-cm
@Temperature 100 °C
0.0000224 ohm-cm
@Temperature 212 °F
annealed specimen
 0.0000300 ohm-cm
@Temperature 200 °C
0.0000300 ohm-cm
@Temperature 392 °F
annealed specimen
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.5 µm/m-°C
@Temperature 20.0 °C
6.39 µin/in-°F
@Temperature 68.0 °F
Typical steel
 12.2 µm/m-°C
@Temperature 0.000 - 300 °C
6.78 µin/in-°F
@Temperature 32.0 - 572 °F
Typical for steel
 13.9 µm/m-°C
@Temperature 0.000 - 500 °C
7.72 µin/in-°F
@Temperature 32.0 - 932 °F
Typical for steel
Specific Heat Capacity 0.486 J/g-°C
@Temperature >=100 °C
0.116 BTU/lb-°F
@Temperature >=212 °F
annealed
Thermal Conductivity 51.9 W/m-K360 BTU-in/hr-ft²-°FTypical steel
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.47 - 0.55 %0.47 - 0.55 %
Iron, Fe 98.46 - 98.92 %98.46 - 98.92 %As remainder
Manganese, Mn 0.60 - 0.90 %0.60 - 0.90 %
Phosphorus, P <= 0.040 %<= 0.040 %
Sulfur, S <= 0.050 %<= 0.050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 1050 Steel, cold drawn, high temperature, stress relieved, 50-75 mm (2-3 in) round
AISI 1050 Steel, cold drawn, low temperature, stress relieved, 22-32 mm (0.875-1.25 in) round
AISI 1050 Steel, cold drawn, low temperature, stress relieved, 50-75 mm (2-3 in) round
AISI 1050 Steel, oil quenched 845°C (1550°F), 540°C (1000°F) temper, 13 mm (0.5 in.) round
AISI 1050 Steel, cold drawn, high temperature, stress relieved, 32-50 mm (1.25-2 in) round

M105AP / 7015

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.