MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

ASI® Debonder for Cyanoacrylate
Categories: Fluid; Solvent

Material Notes: REMOVE DEBONDER is a versatile adhesive remover. This material will remove adhesive from work stations, can be used on a wide range of surfaces, and can be used as a flushing solvent for dispensing systems. It is recommended that before use on a finished party, try the REMOVE DEBONDER on a small area to make sure that the surface is compatible. REMOVE DEBONDER is a single component, solvent based material. It is flammable and the normal precautions used in handling flammable materials should be followed. Mild odor.

Information provided by Adhesive Systems, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 5.0 cP5.0 cP
 
Thermal PropertiesMetricEnglishComments
Boiling Point 38.3 °C101 °F
Flash Point 35.6 °C96.0 °F
 
Descriptive Properties
Color / appearanceclear/amber

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASINC9079 / 233446

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.