MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aclo Accutech Polypropylene Homopolymer HP0336M20CL Mica Reinforced Coupled
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Mica Filler

Material Notes:

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 g/cc0.0368 lb/in³ASTM D792
Linear Mold Shrinkage 0.0080 cm/cm0.0080 in/inMD; ASTM D955
Melt Flow 8.0 g/10 min8.0 g/10 minASTM D1238
Ash 20 %20 %ASTM D2584
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 7474ASTM D785
Tensile Strength at Break 30.0 MPa4350 psiASTM D638
Tensile Strength, Yield 35.0 MPa5080 psiASTM D638
Elongation at Break 15 %15 %ASTM D638
Elongation at Yield 6.0 %6.0 %ASTM D638
Tensile Modulus 2.40 GPa348 ksiASTM D638
Flexural Strength 46.0 MPa6670 psiASTM D790
Flexural Modulus 2.60 GPa377 ksiASTM D790
Izod Impact, Notched 0.422 J/cm0.790 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 123 °C253 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 68.9 °C156 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aclo Accutech Polypropylene Copolymer CP0436C40L1 Calcium Reinforced
Bamberger Polymers Bapolene® 4062NA Polypropylene, Injection Grade
Bamberger Polymers Bapolene® 4072 Polypropylene, Injection Grade
Bamberger Polymers Bapolene® 4082 Polypropylene, Injection Grade
Bamberger Polymers Bapolene® 5063C Polypropylene, Injection Grade

PACLO212 / 22467

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.