MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mocom (ALBIS) ALTECH® PS-HI A 1000/100 Polystyrene, Impact Modified
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Base Polymer: Polystyrene, impact

Special Features: Injection molding grade

Market Segment: Lighting, Packaging, various

Application Area: Fixtures/fittings, various

Typical Applications: Light switches, functional components, various

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ISO 1183
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
@Time 86400 sec
0.0040 - 0.0070 in/in
@Time 24.0 hour
ISO 294-4
Melt Flow 11 g/10 min
@Load 5.00 kg,
Temperature 200 °C
11 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Storage Temperature <= 30.0 °C<= 86.0 °Fdry, protected from light
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 85.0 MPa12300 psiH358/30; ISO 2039-1
Tensile Strength 22.0 MPa3190 psiISO 527
Tensile Strength, Yield 22.0 MPa3190 psiISO 527
Elongation at Break 35 %35 %ISO 527
Elongation at Yield 2.0 %2.0 %ISO 527
Tensile Modulus 1.80 GPa261 ksiISO 527
Flexural Strength 40.0 MPa5800 psiISO 178
Flexural Modulus 1.90 GPa276 ksiISO 178
Charpy Impact Unnotched 10.0 J/cm²47.6 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.900 J/cm²4.28 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C158 °FISO 75-1/-2
Vicat Softening Point 90.0 °C194 °FB50; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 - 260 °C356 - 500 °FInjection molding
Mold Temperature 10.0 - 70.0 °C50.0 - 158 °FInjection molding
Drying Temperature  60.0 - 80.0 °C
@Time 7200 - 10800 sec
140 - 176 °F
@Time 2.00 - 3.00 hour
in a dry air (desiccant) dryer
 60.0 - 80.0 °C
@Time 7200 - 10800 sec
140 - 176 °F
@Time 2.00 - 3.00 hour
air circulating dryer
 
Descriptive Properties
Base PolymerPolystyrene, impact

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyetherimide (PEI)
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
Overview of materials for Nylon 46, Unreinforced
Overview of materials for Liquid Crystal Polymer (LCP), Unfilled
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled

PALBIS8883 / 242942

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.