MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Zeon Specialty Materials Zeonex® RS820 Cyclo Olefin Optical Grade Polymer  (discontinued **)
Categories: Polymer; Thermoplastic; Cyclo Olefin Polymer

Material Notes: Pencil hardness (JIS K5401) is 'B'. White and opaque. Key characteristics of Zeonex® RS820 include high impact resistance; applicable for plating. Major applications include electric insulating parts.

General Zeonex® Information: Specific grades of Zeonex® are available for different applications. Zeonex® features include chemical resistance to acids and bases, low impurity content, and easy processing through injection molding, blow molding, and film extrusion. Specific grades are used in camera lenses, prisms, and VTR lenses; CD pickup lenses, LBP FΘ lenses, and polygon mirrors; films; and other uses in the electric, electronic, medical treatment, and optronics fields.

Information provided by Zeon Chemicals L.P.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³ASTM D792
Water Absorption <= 0.010 %<= 0.010 %ASTM D570
Moisture Vapor Transmission 0.380 cc-mm/m²-24hr-atm0.965 cc-mil/100 in²-24hr-atmg-mm/m²-24 hr; (100µm) JIS Z 0208
Melt Flow 9.0 g/10 min9.0 g/10 min280°C/2.16 kg; JIS K 6719
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 42.0 MPa6090 psiASTM D638
Elongation at Break 100 %100 %ASTM D638
Tensile Modulus 1.90 GPa276 ksiASTM D638
Flexural Yield Strength 57.0 MPa8270 psiASTM D790
Flexural Modulus 1.70 GPa247 ksiASTM D790
Izod Impact, Notched 0.380 J/cm0.712 ft-lb/in3.2 mm sample; ASTM D256
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cmASTM D257
Dielectric Constant 2.27
@Frequency 1e+6 Hz
2.27
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 40.0 kV/mm1020 kV/in1 mm; short time; ASTM D149
Dissipation Factor 0.00020
@Frequency 1e+6 Hz
0.00020
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.0 µm/m-°C
@Temperature 20.0 °C
38.9 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 123 °C253 °FUnannealed; ASTM D648
Glass Transition Temp, Tg 138 °C280 °FDSC
Flammability, UL94 HBHB

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PZEONA / 72961

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.