MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ASI® AS203 Anti-Seize Lubricant
Categories: Fluid; Lubricant

Material Notes: AS203 is a premium quality anti-seize lubricant especially designed to offer the maximum protection of components that are exposed to extremely harsh environments. AS203 offers the greatest resistance to the most corrosive and extreme temperature environments (2600 F). This material is formulated using pure colloidal nickel and graphite flakes that are dispersed in a superior high performance petroleum carrier. AS203 is safe to use with anhydrous ammonia, acetylene, and other vinyl monomers. It will not poison catalyst beds, reaction chambers or special alloy fittings. It does not contain any copper, lead, or molydisulfide. AS203 retards galvanic action.

Information provided by Adhesive Systems, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/cc
Density 1.23 g/cc0.0446 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Penetration 320 - 340320 - 340
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 2.0 %2.0 %
Nickel, Ni 21 %21 %
 
Descriptive Properties
Color / appearanceMetallic Gray
Graphite (%)15
Oil Separation<1% @ 158 F, 30hrs.
Solid Lubricants (%)38

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASINC9217 / 233583

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.