MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Granite
Categories: Ceramic

Material Notes: Granite is an igneous rock with a mixed texture and grain size > 3 mm (plutonic). It is acidic, with a total silica content greater than 65%. The critical mineral of granite is quartz (5-35%); and also contains orthoclase feldspar, plagioclase feldspar, and smaller amounts of biotite.

Granite is used in architecture and construction because it is common and can possess a variety of textures and colors.

Property values are typical of Granite used in construction. Actual property values will vary from sample to sample.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 2.54 - 2.66 g/cc0.0918 - 0.0961 lb/in³
Moisture Expansion 0.005 %0.005 %Bionite granite; Source: Barre, VT, USA
Porosity 0.1 - 4 %0.1 - 4 %
Permeability 1.0e-9 - 1.0e-61.0e-9 - 1.0e-6Aggregation property, d (µ = (-log d))
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore H 85 - 10085 - 100
Hardness, Mohs 5 - 75 - 7
Abrasive Hardness 37 - 8837 - 88
Tensile Strength, Ultimate 7.00 - 25.0 MPa1020 - 3630 psi
Modulus of Elasticity 20.0 - 60.0 GPa2900 - 8700 ksi
Modulus of Rupture 0.00900 - 0.0379 GPa1.31 - 5.50 ksi
Transverse Strength 9.00 - 38.0 MPa1310 - 5510 psi
Compressive Strength 96.5 - 310 MPa14000 - 45000 psi
Impact Toughness 2.76 - 11.0 cm/cm²7.00 - 28.0 in/in²
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 10000 - 1.00e+9 ohm-cm10000 - 1.00e+9 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 3.70 - 11.0 µm/m-°C
@Temperature 20.0 °C
2.06 - 6.11 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 0.210 - 0.350 J/g-°C0.0502 - 0.0837 BTU/lb-°F
Thermal Conductivity 1.20 - 4.20 W/m-K8.33 - 29.1 BTU-in/hr-ft²-°F

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Portland Cement
Aluminum, Al
Verde Fuoco Metasomatite Architectural Stone
Aluminum 6061-T6; 6061-T651
Shale

BMIN050 / 197

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.