MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AGC Fluon® P-830UP PFA Perfluoropolymer
Categories: Polymer; Thermoplastic; Fluoropolymer; Perfluoroalkoxy (PFA); Polyperfluoroalkoxyethylene, Molded/Extruded

Material Notes: Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent characteristics and similar properties of PTFE but can be processed using conventional thermoplastic techniques, such as extrusion molding, injection molding, blow molding, or electrostatic powder coating. And Fluon® PFA can be used in a wide range of temperatures from extremely low to high temperatures (260°C at the maximum) without losing its superior properties.

Information provided by Asahi Glass Company, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.12 - 2.17 g/cc2.12 - 2.17 g/ccASTM D792
Water Absorption <= 0.030 %<= 0.030 %ASTM D570
Melt Flow 24 - 36 g/10 min24 - 36 g/10 min
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6060ASTM D1706
Tensile Strength at Break 32.0 MPa4640 psiASTM D638
Tensile Strength, Ultimate 7.00 MPa
@Temperature 250 °C
1020 psi
@Temperature 482 °F
ASTM D638
Elongation at Break 410 %410 %ASTM D638
 580 %
@Temperature 250 °C
580 %
@Temperature 482 °F
ASTM D638
Flexural Modulus 0.600 GPa87.0 ksiASTM D790
Izod Impact, Notched NBNBASTM D256A
Coefficient of Friction, Dynamic 0.200.20
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+18 ohm-cm>= 1.00e+18 ohm-cmASTM D257
Surface Resistance >= 1.00e+17 ohm>= 1.00e+17 ohmASTM D257
Dielectric Constant  <= 2.1
@Frequency 60 Hz
<= 2.1
@Frequency 60 Hz
ASTM D150
 <= 2.1
@Frequency 1000 Hz
<= 2.1
@Frequency 1000 Hz
ASTM D150
 <= 2.1
@Frequency 1e+6 Hz
<= 2.1
@Frequency 1e+6 Hz
ASTM D150
Dissipation Factor  <= 0.00020
@Frequency 60 Hz
<= 0.00020
@Frequency 60 Hz
ASTM D150
 <= 0.00020
@Frequency 1000 Hz
<= 0.00020
@Frequency 1000 Hz
ASTM D150
 <= 0.00020
@Frequency 1e+6 Hz
<= 0.00020
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance >= 300 sec>= 300 secASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear 130 µm/m-°C
@Temperature 20.0 °C
72.2 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Specific Heat Capacity 1.046 J/g-°C0.2500 BTU/lb-°F
Thermal Conductivity 0.251 W/m-K1.74 BTU-in/hr-ft²-°FASTM C177
Melting Point 300 - 310 °C572 - 590 °F
Maximum Service Temperature, Air 260 °C500 °FContinuous
Flammability, UL94 V-0V-0
Oxygen Index >= 95 %>= 95 %ASTM D2863
 
Descriptive Properties
Flex Life, Cycles18000

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese FORTRON 11400000000 PPS, 40% Glass Reinforced
AGC Fluon® P-805UP PFA Perfluoropolymer
DIAB Klegecell® TR 55 High-performance Expanded Polymer Foam Core Material
Daikin NEOFLON® NP-20 FEP
Chemours Teflon® PFA Grade 950 HP Plus Extrusion and Molding Resin

PAGC83 / 23042

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.