MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Styrodur® 3035 CN Extruded Rigid Polystyrene Foam (Europe)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. The key features of Styrodur C are high compressive strength, low water absorption, and outstanding thermal insulation. It is also rot-proof and easy to handle on site. Compressive strength is the major factor that differentiates the various grades of Styrodur C.

Applications: Cavity walls, Pitched roofs, Ceilings, and Warehouse

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0300 g/cc0.00108 lb/in³
Water Absorption 0.20 %0.20 %by immersion; DIN EN 12087
 <= 3.0 %<= 3.0 %by diffusion; DIN EN 12088
Water Vapor Transmission 100 - 150 g/m²/day6.44 - 9.66 g/100 in²/dayDIN EN 12086
Deformation <= 5.0 %
@Pressure 0.0400 MPa,
Temperature 70.0 °C
<= 5.0 %
@Pressure 5.80 psi,
Temperature 158 °F
DIN EN 1605
 
Mechanical PropertiesMetricEnglishComments
Creep Strength 0.100 MPa
@Strain <=2 %
14.5 psi
@Strain <=2 %
Compressive; DIN EN 1606
Compressive Strength 0.250 MPa
@Strain 10 %
36.3 psi
@Strain 10 %
DIN EN 826
Compressive Modulus 0.0150 GPa2.18 ksiElasticity; Short term E; DIN EN 826
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 80.0 µm/m-°C44.4 µin/in-°FDIN 53752
CTE, linear, Transverse to Flow 60.0 µm/m-°C33.3 µin/in-°FDIN 53752
Thermal Conductivity 0.0330 W/m-K0.229 BTU-in/hr-ft²-°FMoisture Content: 0%
 0.0340 W/m-K0.236 BTU-in/hr-ft²-°FMoisture Content: 1%
 0.0340 W/m-K0.236 BTU-in/hr-ft²-°FMoisture Content: 2%
 0.0350 W/m-K0.243 BTU-in/hr-ft²-°FMoisture Content: 3%
 0.0350 W/m-K0.243 BTU-in/hr-ft²-°FMoisture Content: 4%
 0.0360 W/m-K0.250 BTU-in/hr-ft²-°FMoisture Content: 5%
 0.0370 W/m-K0.257 BTU-in/hr-ft²-°FMoisture Content: 6%
 0.0380 W/m-K0.264 BTU-in/hr-ft²-°FMoisture Content: 8%
 0.0390 W/m-K0.271 BTU-in/hr-ft²-°FMoisture Content: 10%
 0.0400 W/m-K0.278 BTU-in/hr-ft²-°FMoisture Content: 12%
 0.0240 W/m-K
@Temperature -80.0 °C
0.167 BTU-in/hr-ft²-°F
@Temperature -112 °F
 0.0260 W/m-K
@Temperature -60.0 °C
0.180 BTU-in/hr-ft²-°F
@Temperature -76.0 °F
 0.0280 W/m-K
@Temperature -40.0 °C
0.194 BTU-in/hr-ft²-°F
@Temperature -40.0 °F
 0.0300 W/m-K
@Temperature -20.0 °C
0.208 BTU-in/hr-ft²-°F
@Temperature -4.00 °F
 0.0320 W/m-K
@Temperature 0.000 °C
0.222 BTU-in/hr-ft²-°F
@Temperature 32.0 °F
 0.0330 W/m-K
@Temperature 10.0 °C
0.229 BTU-in/hr-ft²-°F
@Temperature 50.0 °F
 0.0340 W/m-K
@Temperature 20.0 °C
0.236 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 0.0350 W/m-K
@Temperature 30.0 °C
0.243 BTU-in/hr-ft²-°F
@Temperature 86.0 °F
 0.0360 W/m-K
@Temperature 40.0 °C
0.250 BTU-in/hr-ft²-°F
@Temperature 104 °F
 0.0370 W/m-K
@Temperature 50.0 °C
0.257 BTU-in/hr-ft²-°F
@Temperature 122 °F
 0.0310 W/m-K
@Thickness 30.0 mm
0.215 BTU-in/hr-ft²-°F
@Thickness 1.18 in
DIN EN 13164
 0.0320 W/m-K
@Thickness 40.0 mm
0.222 BTU-in/hr-ft²-°F
@Thickness 1.57 in
DIN EN 13164
 0.0330 W/m-K
@Thickness 50.0 mm
0.229 BTU-in/hr-ft²-°F
@Thickness 1.97 in
DIN EN 13164
 0.0340 W/m-K
@Thickness 60.0 mm
0.236 BTU-in/hr-ft²-°F
@Thickness 2.36 in
DIN EN 13164
 0.0350 W/m-K
@Thickness 80.0 mm
0.243 BTU-in/hr-ft²-°F
@Thickness 3.15 in
DIN EN 13164
Maximum Service Temperature, Air 75.0 °C167 °FDIN EN 14706
 
Descriptive Properties
Commercial StatusEurope
Dimensional Stability at Heat< 5%70°C, 90% rh; DIN EN 1604
Freeze-Thaw-Resistance<1%DIN EN1209

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe)
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe)
BASF Neopor® 2300 Expandable Polystyrene
BASF Styropor® F 215 T-N Expandable Polystyrene
Versalis Extir® LN 2000 Expandable Polystyrene

PBASG0089 / 131723

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.