MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Plenco 6500 Phenolic, Briquette, Injection Molded
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Novolac, Glass/Flock Filled

Material Notes: PLENCO 06500 is a glass reinforced phenolic molding compound offering improved strength, dimensional stability, and excellent electrical properties. UL recognized under component file E40654. 06500 is available in black.

Information supplied by Plenco.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.720 g/cc0.0260 lb/in³ASTM D1895
Density 1.77 g/cc0.0639 lb/in³ASTM D792
Water Absorption 0.099 %0.099 %ASTM D570
Linear Mold Shrinkage 0.0031 cm/cm0.0031 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 9696ASTM D785
Tensile Strength, Ultimate 78.0 MPa11300 psiASTM D638
Elongation at Break 0.77 %0.77 %ASTM D638
Tensile Modulus 13.3 GPa1930 ksiASTM D638
Flexural Strength 131 MPa19000 psiASTM D790
Flexural Modulus 12.7 GPa1840 ksiASTM D790
Compressive Strength 214 MPa31000 psiASTM D695
Izod Impact, Notched 0.340 J/cm0.637 ft-lb/inASTM D256
Charpy Impact, Notched 0.296 J/cm²1.41 ft-lb/in²ASTM D256
Impact 177177J/m Drop Ball Impact; PLENCO
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.30e+11 ohm-cm5.30e+11 ohm-cmASTM D247
Dielectric Constant 5.05.0ASTM D150
Dielectric Strength 8.40 kV/mm213 kV/inStep by Step; ASTM D149
 20.9 kV/mm531 kV/inShort Time; ASTM D149
Dissipation Factor 0.0330.033ASTM D150
Arc Resistance 159 sec159 secASTM D495
Comparative Tracking Index 175 V175 VASTM D3638
 
Thermal PropertiesMetricEnglishComments
CTE, linear 35.0 µm/m-°C
@Temperature 40.0 - 130 °C
19.4 µin/in-°F
@Temperature 104 - 266 °F
TMA; ASTM E831
Thermal Conductivity 0.540 W/m-K
@Temperature 100 °C
3.75 BTU-in/hr-ft²-°F
@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 194 °C381 °FHeat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 196 °C385 °FASTM D648
Flammability, UL94 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
Oxygen Index 34 %34 %ASTM D2863
Shrinkage 0.084 %0.084 %72 hr, 120ºC; ASTM D1299

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Plenco 2535 Phenolic, Granular, Injection Molded
Plenco 00757 Melamine-Phenolic, Granular, Injection Molded
Plenco 00755 Melamine-Phenolic, Granular, Injection Molded
Plenco 00732 Melamine-Phenolic, Granular, Injection Molded
Plenco 00714 Melamine-Phenolic, Granular, Injection Molded

PLEM12 / 50691

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.