MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Chevron Phillips Marlex® D173 Film Grade LLDPE
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Hexene, Film Grade

Material Notes: This metallocene linear low density polyethylene is an ethylene-hexene copolymer tailored for cast film applications that require:
  • Superior clarity
  • Excellent gloss
  • Exceptional toughness
  • Outstanding heat seal
Typical cast film applications include:
  • Stretch wrap
  • Overwrap
  • Coextrusions

Information provided by Chevron Phillips Chemical Company LP.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.918 g/cc0.0332 lb/in³ASTM D1505
Melt Flow 3.50 g/10 min
@Load 2.16 kg,
Temperature 190 °C
3.50 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 10.0 MPa1450 psiASTM D882
Film Tensile Strength at Yield, TD 9.00 MPa1310 psiASTM D882
Film Elongation at Break, MD 500 %500 %ASTM D882
Film Elongation at Break, TD 580 %580 %ASTM D882
Coefficient of Friction >= 1.00>= 1.00ASTM D1894
Elmendorf Tear Strength, MD 11.8 g/micron300 g/milASTM D1922
Elmendorf Tear Strength, TD 19.7 g/micron500 g/milASTM D1922
Dart Drop 17.7 g/micron450 g/milASTM D1709
Film Tensile Strength at Break, MD 54.0 MPa7830 psiASTM D882
Film Tensile Strength at Break, TD 38.0 MPa5510 psiASTM D882
1% Secant Modulus, MD 103 MPa14900 psiASTM D882
1% Secant Modulus, TD 110 MPa16000 psiASTM D882
Heat Seal Strength Initiation Temperature 101 °C214 °FASTM F88
 
Optical PropertiesMetricEnglishComments
Haze 2.00 %2.00 %ASTM D1003
Gloss 140 %140 %60°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHEVC8810 / 323313

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.