MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Borealis Borlink™ LE4212 Scorch Retardant, Crosslinkable Polyethylene, Water Tree Retardant Insulation for Me Power Cables
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Wire/Cable Grade

Material Notes: LE4212 is a natural, crosslinkable low density polyethylene compound, which has water tree retardant and scorch retardant properties. LE4212 has been specifically developed as a scorch retardant, water tree retardant insulation for long life, medium voltage power cables. Because it is a Superclean material, it can be used for voltages up to 276kV.

Former trade name for this product was SuperTR™.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.923 g/cc0.0333 lb/in³Base Resin; ASTM D1928/D 1505
Degree of Crosslinking 12 %12 %ASTM D2765
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5050ASTM D2240
Tensile Strength, Yield >= 14.3 MPa>= 2070 psiHeat Aging (168 hrs at 136°C); ASTM D638
 15.9 MPa2300 psiAt 20 in/min; ASTM D638
Elongation at Break <= 75 %<= 75 %Hot Creep Test (150°C,29 psi); ICEA T-28-562
 360 %360 %Heat Aging (168 hrs at 136°C); ASTM D412
 400 %400 %ASTM D638
Tensile Set 5.0 %5.0 %Hot Creep Test (150°C,29 psi); ICEA-T-28-562
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Dielectric Constant <= 2.3
@Frequency 50 Hz
<= 2.3
@Frequency 50 Hz
ASTM D150
Dielectric Strength >= 21.7 kV/mm>= 550 kV/inASTM D149
Dissipation Factor 0.00050
@Frequency 50 Hz
0.00050
@Frequency 50 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -76.0 °C<= -105 °FASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis FL5580 High Density Polyethylene
Borealis Borlink™ LE0595 Crosslinkable Semiconductive Compound for Shielding of Power Cables
Borealis Borlink™ LE0594 Crosslinkable Semiconductive Compound for Shielding of Power Cables
Borealis Casico™ FR4807 Non-Halogen Flame Retardant Compound for Low Voltage Insulation and Jacketing
Borealis Casico™ FR4805 Non Halogen Flame Retardant Compound for Sheathing Energy Cables

PBOREA189 / 27496

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.