MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mitsubishi Iupiace® AP6GM4 m-Polyphenylene Ether (m-PPE)
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polyphenylene Ether, 20% Glass Filled

Material Notes: 20% reinforced GF+filler. High flowabillity V1 grade. Iupiace is a polymer alloy made by modifying PPE with high impact polystyrene (HIPS), nylon-6 or nylon-66. Usability in a wide range of temperatures (-40 to 160). Higher rigidity, impact strength and fatigue resistance. Excellent insulation properties, low dielectric constant and low dielectric dissipation factor. Excellent dimensional stability with low water absorption. Flame retardance and excellent self-extinguishing properties. Low density. Low shrinkage rate, ensuring quality precision parts. Good mold release, easy flow properties and a wide range of stock temperatures.

Information provided by Mitsubishi Engineering Plastics Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³ISO 1183
Water Absorption 0.060 %
@Temperature 23.0 °C
0.060 %
@Temperature 73.4 °F
Immersion
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm
@Thickness 3.20 mm
0.0020 - 0.0040 in/in
@Thickness 0.126 in
Linear Mold Shrinkage, Transverse 0.0030 - 0.0050 cm/cm
@Thickness 3.20 mm
0.0030 - 0.0050 in/in
@Thickness 0.126 in
Melt Flow 31 g/10 min
@Load 5.00 kg,
Temperature 280 °C
31 g/10 min
@Load 11.0 lb,
Temperature 536 °F
cm³/10 min Volumetric Rate; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 80.0 MPa11600 psiISO 527-1,2
Elongation at Break 2.7 %2.7 %ISO 527-1,2
Tensile Modulus 5.70 GPa827 ksiISO 527-1,2
Flexural Strength 132 MPa19100 psiISO 178
Flexural Modulus 5.50 GPa798 ksiISO 178
Charpy Impact, Notched 0.600 J/cm²2.86 ft-lb/in²ISO 179-1,2
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.00e+15 ohm-cm5.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+15 ohm1.00e+15 ohmIEC 60093
Dielectric Constant  3.1
@Frequency 1e+6 Hz
3.1
@Frequency 1e+6 Hz
IEC 60250
 3.2
@Frequency 100 Hz
3.2
@Frequency 100 Hz
IEC 60250
Dielectric Strength  18.0 kV/mm
@Thickness 1.00 mm
457 kV/in
@Thickness 0.0394 in
IEC 60243-1
 18.0 kV/mm
@Thickness 3.00 mm
457 kV/in
@Thickness 0.118 in
IEC 60243-1
Dissipation Factor  0.0057
@Frequency 100 Hz
0.0057
@Frequency 100 Hz
IEC 60250
 0.0067
@Frequency 1e+6 Hz
0.0067
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 200 V200 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 37.0 µm/m-°C20.6 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 68.0 µm/m-°C37.8 µin/in-°FISO 11359-2
Maximum Service Temperature, Air 160 °C320 °F
Deflection Temperature at 1.8 MPa (264 psi) 115 °C239 °FISO 75-1,2
Minimum Service Temperature, Air -40.0 °C-40.0 °F
Flammability, UL94 V-1
@Thickness 1.50 mm
V-1
@Thickness 0.0591 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Iupiace® EHM103R m-Polyphenylene Ether (m-PPE)
BASF Luranyl® KR 2403 G2 Polyphenylene Ether + Styrene-Butadiene Blend, 10% Glass Fiber Reinforced
Mitsubishi Iupiace® AP6GM2 m-Polyphenylene Ether (m-PPE)
Mitsubishi Iupiace® LGX420N m-Polyphenylene Ether (m-PPE)
Mitsubishi Iupiace® AP4GM6 m-Polyphenylene Ether (m-PPE)

PMITSU9094 / 191767

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.