MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik Lauramid® A Nylon 12G
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, Cast

Material Notes: LAURAMID A exhibits, due to its very low water absorption, very good hydrolysis resistance: good dimensional stability, tear resistance and chemical resistance.

Applications: Metal composites for cogs, sprockets and spiral drive wheels, rolls, propellers, metal composite profiles, other profiles, seals.

ISO data as provided by the manufacturer.

Key Words: Polyamide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.03 g/cc0.0372 lb/in³
Water Absorption 1.0 %1.0 %
Moisture Absorption at Equilibrium <= 0.50 %<= 0.50 %Humidity Absorption
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 60.0 MPa8700 psi
Elongation at Break 11 %11 %
Elongation at Yield 9.0 %9.0 %
Modulus of Elasticity 2.10 GPa305 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 3.00e+14 ohm-cm3.00e+14 ohm-cm
Surface Resistance 1.00e+14 ohm1.00e+14 ohm
Dielectric Constant 3.0
@Frequency 100 Hz
3.0
@Frequency 100 Hz
Dissipation Factor 0.038
@Frequency 100 Hz
0.038
@Frequency 100 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear <= 50.0 µm/m-°C
@Temperature 20.0 °C
<= 27.8 µin/in-°F
@Temperature 68.0 °F
Deflection Temperature at 1.8 MPa (264 psi) 175 °C347 °F
Vicat Softening Point 180 °C356 °F50°C/hr/50 N

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EMS-Grivory Grilamid® TR 55 PA12/MACMI
Evonik Lauramid® B Nylon 12G
EMS-Grivory Grilamid® LM-05 HX nat PA12
Evonik Vestamid® L1940 Nylon 12
Evonik Vestamid® X7166 Flame Retardant Nylon 12

PHUL03 / 47263

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.