MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Röchling Glastic Laminates/Shapes TSF Fiberglass-Reinforced Polyester Laminate
Categories: Polymer; Thermoset; Composite SMC; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester Glass Filled BMC

Material Notes: Data provided by Glastic Corporation.

NEMA GPO-1. General purpose, high impact, heat resistant, dimensionally stable, cold punching. Excellent hot compression.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 154 MPa22300 psi
 
Electrical PropertiesMetricEnglishComments
Arc Resistance 127 sec127 secASTM D495
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 155 °C311 °FNEMA temperature
UL RTI, Electrical 130 °C266 °F
UL RTI, Mechanical with Impact 130 °C266 °F
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Röchling Glastic Laminates/Shapes HIR Grade HIR Fiberglass-Reinforced Polyester Rod
Röchling Glastic T-160 Fiberglass-Reinforced Polyester Laminate
Röchling Glastic Laminates/Shapes UTR Pultruded Tubing, Fiberglass-Reinforced Polyester
Röchling Glastic Laminates/Shapes UTS Fiberglass-Reinforced Polyester Laminate
Quantum Composites QC-8800 63% Glass Fiber Vinyl Ester SMC

PGLASV / 41932

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.