MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Syensqo (Solvay Specialty Polymers) Tribocomp® PA66 AF15 TS0 Aramid fiber reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Aramid Fiber Filled

Material Notes: Aramid fiber reinforced PA66, heat stabilized, friction & wear modified. It can easily be processed on most injection molding machines.

Tribocomp® PA66 AF15 TS0 is an aramid fiber reinforced PA66 that is heat stabilized and friction and wear modified. It can easily be processed on most injection molding machines.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³ISO 1183
Moisture Absorption 1.60 %1.60 %50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0080 cm/cm0.0080 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield  35.0 MPa
@Temperature 120 °C
5080 psi
@Temperature 248 °F
ISO 527-2
 45.0 MPa
@Temperature 90.0 °C
6530 psi
@Temperature 194 °F
ISO 527-2
 85.0 MPa
@Temperature 23.0 °C
12300 psi
@Temperature 73.4 °F
ISO 527-2
Elongation at Break 5.0 %5.0 %ISO 527-2
Tensile Modulus  0.850 GPa
@Temperature 120 °C
123 ksi
@Temperature 248 °F
ISO 527-2
 1.20 GPa
@Temperature 90.0 °C
174 ksi
@Temperature 194 °F
ISO 527-2
 4.20 GPa
@Temperature 23.0 °C
609 ksi
@Temperature 73.4 °F
ISO 527-2
Flexural Strength 105 MPa15200 psiISO 178
Flexural Modulus 3.40 GPa493 ksiISO 178
Charpy Impact Unnotched 3.00 J/cm²14.3 ft-lb/in²ISO 179
Charpy Impact, Notched 0.500 J/cm²2.38 ft-lb/in²ISO 179
Coefficient of Friction, Dynamic 0.130.13vs. Itself; ASTM D1894
Coefficient of Friction, Static 0.130.13vs. Itself; ASTM D1894
K (wear) Factor 14.0 x 10-8 mm³/N-M6.95 x 10-10 in³-min/ft-lb-hrASTM D3702
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 30.0 kV/mm762 kV/inIEC 60243-1
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 50.0 µm/m-°C27.8 µin/in-°FISO 11359-2
Thermal Conductivity 0.230 W/m-K1.60 BTU-in/hr-ft²-°FISO 8302
Deflection Temperature at 0.46 MPa (66 psi) 245 °C473 °FUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 190 °C374 °FUnannealed; ISO 75-2/A
 
Processing PropertiesMetricEnglishComments
Zone 1 270 - 300 °C518 - 572 °FExtrusion
Zone 2 275 - 295 °C527 - 563 °FExtrusion
Zone 3 270 - 295 °C518 - 563 °FExtrusion
Zone 4 280 - 310 °C536 - 590 °FExtrusion
 
Descriptive Properties
AdditivePTFE Lubricant
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorBlack
FormsPellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4559 / 280359

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.