MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mid-Mountain Materials CERMEX® MT1800 Needled Silica Mat
Categories: Ceramic; Glass; Glass Fiber; Oxide; Silicon Oxide; Other Engineering Material; Composite Fibers

Material Notes: CERMEX® MT1800 Needled Silica Blanket is a binderless material comprised of high purity, amorphous silica fibers. In demanding applications, the abrasion and vibration resistance of this mat makes this material superior to other products manufactured from shot-containing fibers. The complete absence of shot and organic binders make this product superior in performance in severe environments where vibration can often degrade shot containing materials. The amorphous silica fibers that make up CERMEX® MT1800 mat are unaffected by most chemicals, except strong alkalis, hydrofluoric acid or sodium. Inherent to the chemistry, the silica fibers will have a tendency to shrink on initial exposure to elevated temperatures. For most industrial applications, this does not pose a problem. However, in applications where dimensional stability is critical (at elevated temperatures), CERMEX® MT1800 is available in a pre-shrunk (fired) version.

Information provided by Mid-Mountain Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.136 - 0.152 g/cc0.00492 - 0.00550 lb/in³
Filament Diameter 6.0 - 9.0 µm6.0 - 9.0 µm
Thickness 6350 microns250 mil
 12700 microns500 mil
 25400 microns1000 mil
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.0648 W/m-K
@Temperature 260 °C
0.450 BTU-in/hr-ft²-°F
@Temperature 500 °F
 0.112 W/m-K
@Temperature 538 °C
0.777 BTU-in/hr-ft²-°F
@Temperature 1000 °F
 0.200 W/m-K
@Temperature 816 °C
1.39 BTU-in/hr-ft²-°F
@Temperature 1500 °F
 0.278 W/m-K
@Temperature 982 °C
1.93 BTU-in/hr-ft²-°F
@Temperature 1800 °F
Melting Point 1704 °C3099 °F
Maximum Service Temperature, Air 982 °C1800 °FContinuous
 1260 °C2300 °FIntermittent
 
Component Elements PropertiesMetricEnglishComments
SiO2 >= 96 %>= 96 %
 
Descriptive Properties
Roll Length (ft)1161/4" (350 ft2/roll)
 331" (100 ft2/roll)
 581/2" (175 ft2/roll)
Shot Content (%)None
Width (in)36

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Microtherm Group Hydrophoblic Quilted Panel Filament Reinforced Silica Thermal Insulation Panel, Flexible and Waterproof
Thermal Ceramics Pyro-Bloc HS Module
Morgan Advanced Ceramics Veneering Modules Pyro-Bloc R Thermal Ceramic
Morgan Advanced Ceramics Sintox ™ FA Mac-A950R-1 Aluminum Oxide Ceramic
Mid-Mountain Materials SILTEX® 18 Amorphous Silica Textile

CMID65 / 141233

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.