MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC CYCOLAC™ DL200H ABS (Americas)
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: CYCOLAC DL200H is a hydrostable high heat ABS/PC blend

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.11 g/cc0.0401 lb/in³ISO 1183
Melt Flow  9.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
9.0 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 25 g/10 min
@Load 5.00 kg,
Temperature 260 °C
25 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 40.0 MPa5800 psi50 mm/min; ISO 527
Tensile Strength, Yield 47.0 MPa6820 psi5 mm/min; ASTM D638
 49.0 MPa7110 psi50 mm/min; ISO 527
Elongation at Break 70 %70 %5 mm/min; ASTM D638
 75 %75 %50 mm/min; ISO 527
Elongation at Yield 3.9 %3.9 %50 mm/min; ISO 527
Tensile Modulus 2.33 GPa338 ksi5 mm/min; ASTM D638
 2.35 GPa341 ksi1mm/min; ISO 527
Flexural Yield Strength 75.0 MPa10900 psi2 mm/min; ISO 178
 77.0 MPa11200 psi1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.10 GPa305 ksi2 mm/min; ISO 178
 2.20 GPa319 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 6.20 J/cm11.6 ft-lb/inASTM D256
 5.00 J/cm
@Thickness 6.40 mm
9.37 ft-lb/in
@Thickness 0.252 in
ASTM D256
Izod Impact, Notched (ISO) 56.0 kJ/m²26.6 ft-lb/in²80*10*4; ISO 180/1A
 21.0 kJ/m²
@Temperature -40.0 °C
9.99 ft-lb/in²
@Temperature -40.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 6.50 J/cm²30.9 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 3.00 J/cm²
@Temperature -30.0 °C
14.3 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 118 °C
@Thickness 3.20 mm
244 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 96.0 °C205 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 96.0 °C
@Thickness 3.20 mm
205 °F
@Thickness 0.126 in
unannealed; ASTM D648
 101 °C
@Thickness 6.40 mm
214 °F
@Thickness 0.252 in
unannealed; ASTM D648
Vicat Softening Point 112 °C234 °FRate B/50; ISO 306
 114 °C237 °FRate B/120; ISO 306
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 260 - 290 °C500 - 554 °FInjection Molding
Zone 1 250 - 280 °C482 - 536 °F
Zone 2 255 - 290 °C491 - 554 °F
Zone 3 255 - 290 °C491 - 554 °F
Melt Temperature 260 - 290 °C500 - 554 °F
Mold Temperature 75.0 - 100 °C167 - 212 °F
Drying Temperature 100 - 105 °C212 - 221 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
 8.00 hour8.00 hourCumulative; Injection Molding
Moisture Content 0.040 %0.040 %
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 30 - 80 %30 - 80 %
Vent Depth 0.00380 - 0.00760 cm0.00150 - 0.00299 in
Screw Speed 40 - 70 rpm40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI10009 / 243476

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.