MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Opti-Polymers Optiform POM-C GF25 ST natural POM, 25% Glass fiber filled
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, 30% Glass Fiber Reinforced

Material Notes: High strength and stiff POM compound with low water absorption.

Information provided by Opti-Polymer

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.56 g/cc0.0564 lb/in³ISO 1183
Maximum Moisture Content 0.20
@Temperature 100 °C,
Time 299 sec
0.20
@Temperature 212 °F,
Time 0.0830 hour
thermogravimetric
Melt Flow 3.0 g/10 min
@Load 5.00 kg,
Temperature 190 °C
3.0 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Ash 23 - 27 %
@Temperature 625 °C
23 - 27 %
@Temperature 1160 °F
ISO 3451
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 50.0 MPa7250 psi5 mm / min; ISO 527-1
Elongation at Break 5.0 %5.0 %5 mm / min; ISO 527-1
Tensile Modulus 7.50 GPa1090 ksi1 mm / min; ISO 527-1
Charpy Impact, Notched 0.500 J/cm²2.38 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 145 °C293 °FISO75-1/-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 165 °C329 °Finjection molding
Mold Temperature 40.0 - 85.0 °C104 - 185 °Finjection molding
Drying Temperature 80.0 °C176 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
 
Descriptive Properties
Regional AvailabilityEurope

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

POPTI049 / 255185

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.