MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Piezo Kinetics PKI 100 Lead Metaniobate Piezoelectric
Categories: Ceramic; Oxide; Piezoelectric

Material Notes: Lead Metaniobate exhibits properties not usually present in other types of piezoelectric ceramics. The noteworthy facts are its low mechanical QM, negligible aging, wide range of operating temperatures and small values for lateral and planar coupling compared to longitudinal coupling. The low QM enhances the use of PKI 100 material in the construction of wide bandwidth sensors for high frequency pulse echo measurements that require a short pulse and critical resolution. Its negligible aging helps simplify circuit design. Wide variations in temperature have limited effect on its dielectric and piezoelectric properties making it ideal for high temperature applications. Its high longitudinal coupling compared to lateral and planar coupling allows it to generate a better response under hydrostatic pressures and makes it useful for underwater sonar equipment.

Property data at 25°C. Information supplied by Piezo Kinetics, Inc.

Key Words: Lead Niobium Oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 6.00 g/cc0.217 lb/in³
 
Electrical PropertiesMetricEnglishComments
Curie Temperature 450 °C842 °F
Dielectric Constant 300
@Frequency 1000 Hz
300
@Frequency 1000 Hz
Dissipation Factor <= 0.015
@Frequency 1000 Hz
<= 0.015
@Frequency 1000 Hz
Piezoelectric Longitudinal Coupling Factor, k33 0.350.35
Piezoelectric Shear Charge Coefficient, d15, 10^-12 m/V 105105
Piezoelectric Longitudinal Voltage Coefficient, g33, 10^-3 V-m/N 3232
Piezoelectric Planar Coupling Factor, kp 0.100.10
Piezoelectric Mechanical Q 2020
Piezoelectric Shear Coupling Factor, k15 0.280.28
Piezoelectric Longitudinal Charge Coefficient, d33, 10^-12 m/V 8585
Piezoelectric Shear Voltage Coefficient, g15, 10^-3 V-m/N 3131
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 350 °C662 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Piezo Kinetics 402 Lead Zirconate Titanate Piezoelectric
Shinil Chemical SHINCON PETG Electro Conductive Polymer
Morgan Advanced Ceramics Piezo Materials for Medical Devices PZT-K5K4 HD Piezoceramic Material
Piezo Kinetics PKI 105 Lead Metaniobate Piezoelectric
Piezo Kinetics PKI 802 Navy Type III Lead Zirconate Titanate Piezoelectric

CPKI00 / 1705

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.