Pharmalene MR 50 PH is a linear low density polyethylene (LLDPE) with antioxidants, obtained by medium pressure autoclave technology. It is produced in conformity to the good manufacturing practices (GMP) and is mainly used for injection molding. Application: Pharmalene MR 50 PH is intended for the use within pharmaceutical sector and is characterized by a high rigidity. Pharmalene MR 50 PH is suitable for the production thin walled pharmaceutical containers as well as closures. Information provided by Versalis. |