Arla Plast MAKROTECH™ is a range of opaque colored polycarbonate sheets. The product is virtually unbreakable with extremely high impact resistance. The product offers high temperature performance too. MAKROTECH™ FR is flame retardant sheet produced with halogen free according to DIN VDE 472 part 815. A yellow card on the base material is also available on the UL website. Benefits: Flame retardant (halogen free); High impact resistance and virtually unbreakable; Wide temperature range Application: Flame retardant requirements (UL 94, oxygen index, glow wire) for indoor flat, curved and formed applications like electrical appliances, machine covers and containers. Information provided by Arla Plast. |