MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Niobium Nb-1Zr (Wah Chang WC-1Zr; Fansteel 80), Reactor Grade
Categories: Metal; Nonferrous Metal; Niobium Alloy; Refractory Metal

Key Words: Columbium Alloy, UNS R04251 (Reactor Grade); ASTM B391; ASTM B392; ASTM B393; ASTM B394
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.59 g/cc0.310 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 159 MPa
@Temperature 1090 °C
23000 psi
@Temperature 2000 °F
Recrystallized
Tensile Strength, Ultimate 241 MPa35000 psiRecrystallized
 160 MPa
@Temperature 1093 °C
23200 psi
@Temperature 1999 °F
Recrystallized prior to test
Tensile Strength, Yield 138 MPa20000 psiRecrystallized
Elongation at Break 20 %20 %in 25 mm; Recrystallized
Rupture Strength 96.5 MPa
@Temperature 1090 °C,
Time 36000 sec
14000 psi
@Temperature 2000 °F,
Time 10.0 hour
Recrystallized
Tensile Modulus 68.9 GPa9990 ksi
Machinability 80 %80 %C36000 Brass as 100%
Shear Strength 250 MPa36300 psiAverage for rivet
Charpy Impact >= 81.0 J>= 59.7 ft-lbV-Notch, as-rolled
 126 J92.9 ft-lbV-Notch, Recrystallized
 160 J118 ft-lbV-Notch, stress-relieved
Charpy Impact, Unnotched 174 J128 ft-lbRecrystallized
 175 J129 ft-lbStress-relieved
 210 J155 ft-lbAs-Rolled
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000147 ohm-cm
@Temperature 0.000 °C
0.00000147 ohm-cm
@Temperature 32.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 7.54 µm/m-°C
@Temperature 20.0 - 408 °C
4.19 µin/in-°F
@Temperature 68.0 - 766 °F
Specific Heat Capacity 0.270 J/g-°C0.0645 BTU/lb-°F
Thermal Conductivity 41.9 W/m-K291 BTU-in/hr-ft²-°F
Melting Point <= 2407 °C<= 4365 °F
Liquidus 2407 °C4365 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.010 %<= 0.010 %
Hafnium, Hf <= 0.010 %<= 0.010 %
Hydrogen, H <= 0.0020 %<= 0.0020 %
Iron, Fe <= 0.0050 %<= 0.0050 %
Molybdenum, Mo <= 0.0050 %<= 0.0050 %
Nickel, Ni <= 0.0050 %<= 0.0050 %
Niobium, Nb (Columbium, Cb) >= 98.5 %>= 98.5 %
Nitrogen, N <= 0.030 %<= 0.030 %
Oxygen, O <= 0.015 %<= 0.015 %
Silicon, Si <= 0.0050 %<= 0.0050 %
Tantalum, Ta <= 0.10 %<= 0.10 %
Tungsten, W <= 0.030 %<= 0.030 %
Zirconium, Zr 0.80 - 1.2 %0.80 - 1.2 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Niobium Nb-1Zr (Wah Chang WC-1Zr; Fansteel 80), Commercial Grade
Goodfellow Niobium 56/Titanium 44 Alloy
Niobium, Nb; High Purity
Niobium, Nb; Unalloyed RG (UNS R04200)
Tungsten Carbide, WC

MRNb01 / 13900

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.