MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Afton Plastics 440HP PFA Compression Molded Rod
Categories: Polymer; Thermoplastic; Fluoropolymer; Perfluoroalkoxy (PFA)

Material Notes: PFA is a high-performance, melt processable fluoropolymer that exhibits similar characteristics to PTFE. It performs exceedingly well in extreme thermal and chemical environments. While originally designed for use in extrusion and injection molding, Afton Plastics processes Chemours Teflon™ PFA 440HP in large diameter, 12” long, compression-molded rod.

Product Benefits: Temperature range: -320°F to +500°F, • Exceptional dielectric insulation properties, • Negligible moisture absorption, • Low coefficient of friction, • Non-stick surface, • Very low gas permeation and outgassing, • May be welded with hot air welding equipment, • Improved thermal stability, • Chemically inert to industrial chemicals and solvents, • High resistance to outdoor weathering, • Does not support combustion, • Low metals and ion extractables.

Application: Pump housings and pipe linings, • Fluid handling or chemical processing equipment, • Wet bench equipment, • Tanks, • Semiconductor wafer carriers, • Life sciences, • Instrumentation for fluidic systems, • Hostile environments involving chemical, thermal, and mechanical stress • Food processing and packing equipment.

Made from Teflon®, a Chemours product, processed into shapes and components by Afton plastics.

Information provided by Afton Plastics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.12 - 2.17 g/cc2.12 - 2.17 g/ccASTM D792
Water Absorption <= 0.030 %
@Time 86400 sec
<= 0.030 %
@Time 24.0 hour
ASTM D570
Melt Flow 12 - 15 g/10 min12 - 15 g/10 minCondition B; ASTM D3307
 14 - 19 g/10 min14 - 19 g/10 minCondition A; ASTM D3307
 18 - 21 g/10 min18 - 21 g/10 minCondition D; ASTM D3307
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5555ASTM D2240
Tensile Strength 24.8 MPa3600 psiASTM D3307
Tensile Strength, Yield 13.8 MPa2000 psiASTM D3307
Elongation at Break 300 %300 %ASTM D3307
Flexural Modulus 0.586 GPa85.0 ksiASTM D790
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+18 ohm-cm1.00e+18 ohm-cmASTM D257
Dielectric Constant 2.03
@Frequency 6.00e+7 Hz
2.03
@Frequency 6.00e+7 Hz
ASTM D150
Dielectric Strength 78.7 kV/mm
@Thickness 10.0 mm
2000 kV/in
@Thickness 0.394 in
short time; ASTM D149
Dissipation Factor 0.00010
@Frequency 6.00e+7 Hz
0.00010
@Frequency 6.00e+7 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear  140 µm/m-°C
@Temperature 21.0 - 100 °C
77.8 µin/in-°F
@Temperature 69.8 - 212 °F
ASTM D696
 170 µm/m-°C
@Temperature 100 - 149 °C
94.4 µin/in-°F
@Temperature 212 - 300 °F
ASTM D696
 210 µm/m-°C
@Temperature 149 - 208 °C
117 µin/in-°F
@Temperature 300 - 406 °F
ASTM D696
Melting Point 302 - 310 °C576 - 590 °FASTM D3418
Maximum Service Temperature, Air 260 °C500 °F
Minimum Service Temperature, Air -196 °C-320 °F
Oxygen Index >= 95 %>= 95 %ASTM D2863

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Afton Plastics 450HP PFA Welding Rod
Afton Plastics 350 PFA Welding Rod
Chemours Teflon® PTFE Grade 30 Aqueous Dispersion
Chemours Teflon® PTFE Grade 313A Aqueous Dispersion
Albis Plastics Tedur® L V 9400-1 PPS, 15% Carbon Fiber

PAFTON904 / 232128

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.