MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Daikin PTFE F-201L Polytetrafluoroethylene Extrusion Grade Fine Powder
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Extruded

Material Notes: Daikin PTFE F-201L is a polytetrafluoroethylene fine powder resin for paste extrusion manufactured without the use of PFOA. F-201L has been designed with low extrusion pressure for spaghetti tubing, thin wall tubing and wire coating applications of less than 16 AWG that are run at high reduction ratios.

Information provided by Daikin.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.16 - 2.20 g/cc2.16 - 2.20 g/ccASTM D 4895
Bulk Density 0.400 - 0.550 g/cc0.0145 - 0.0199 lb/in³ASTM D 4895
Particle Size 400 - 650 µm400 - 650 µmASTM D 4895
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break >= 25.0 MPa>= 3630 psiASTM D 4895
Elongation at Break >= 350 %>= 350 %ASTM D 4895
 
Descriptive Properties
AppearanceWhite Powder
Extrusion Pressure540-650 KgF/cm2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDAIJ9888 / 209959

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.