MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Elvax® 3174 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Cast Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade

Material Notes: 18 wt% Vinyl Acetate.

Elvax® 3174 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.

Additives: Antioxidant.

Applications: Elvax® 3174 is designed to provide a low temperature heat seal to itself or many other materials commonly used in flexible packaging applications. The melt properties of this resin allow it to be processed on cast film equipment over a wide range of line speeds and film thicknesses. It can also be coextruded with a variety of other polymers. Elvax® 3174 is typically used as a low-temperature seal layer in coextruded films.

Information provided by DuPont Packaging Polymers.

This product line/trade name was acquired by Dow, but this specific grade was discontinued prior to the acquisition.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc0.0340 lb/in³ASTM D792
Melt Flow 8.0 g/10 min8.0 g/10 minCondition not noted.; ASTM D1238
 
Thermal PropertiesMetricEnglishComments
Melting Point 65.0 °C149 °FFreezing Point via DSC/ASTM D3418
 86.0 °C187 °FUpon Melting via DSC/ASTM D3418
Vicat Softening Point 61.0 °C142 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Melt Temperature 150 - 205 °C302 - 401 °Fcast film extrusion.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Elvax® 3180Z Ethylene Vinyl Acetate
Dow Elvax® 3175 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion
Dow Elvax® 3200-2 Ethylene-Vinyl Acetate Copolymer Resin for Extrusion Coating
Dow Elvax® 260 Ethylene-Vinyl Acetate Copolymer Resin
Dow Elvax® 3169Z Ethylene Vinyl Acetate

PDUPHJ / 33622

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.