MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

ASI® Pipe Sealer TORQUE 175 Anaerobic Methacrylate Adhesive
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: TORQUE 175 is a medium strength anaerobic sealant for threads connectors up to 1"1/2. To be used in the sealing of gases, water, LPG, hydrocarbons, oils and other chemicals. Cured sealant forms elastic films highly resistant to vibrations and shocks. Retains sealant properties up to 200°C.

Information provided by Adhesive Systems, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³uncured
Viscosity 400 cP
@Temperature 25.0 °C
400 cP
@Temperature 77.0 °F
 
Mechanical PropertiesMetricEnglishComments
Shear Strength 10.0 - 14.0 MPa1450 - 2030 psiZinc plated bolt M 10x20- quality 8.8- nut h=0.8d.; ASTM D1002
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 180 °C356 °FZinc Plated bolt M 10x20 quality 8.8-nut h=0.8d
Minimum Service Temperature, Air -55.0 °C-67.0 °FZinc Plated bolt M 10x20 quality 8.8-nut h=0.8d
Flash Point >= 100 °C>= 212 °Funcured
 
Processing PropertiesMetricEnglishComments
Cure Time 15.0 - 30.0 min0.250 - 0.500 hourHandling, Cured. Zinc plated bolt M 10x20- quality 8.8- nut h=0.8d.
 60.0 - 180 min1.00 - 3.00 hourFunctional Cure. Zinc plated bolt M 10x20- quality 8.8- nut h=0.8d.
 720 - 1440 min12.0 - 24.0 hourFull Cure. Zinc plated bolt M 10x20- quality 8.8- nut h=0.8d.
Shelf Life 12.0 Month
@Temperature <=28.0 °C
12.0 Month
@Temperature <=82.4 °F
uncured
 
Descriptive Properties
Chemical ClassAnaerobic Methacrylate
Color / appearancered
Locking Torque18-28 N.m. Breakaway. ISO 10964. Zinc Plated bolt M 10x20 quality 8.8-nut h=0.8d
 18-28 N.m. Prevailing. ISO 10964. Zinc Plated bolt M 10x20 quality 8.8-nut h=0.8d

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASINC9188 / 233554

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.