MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nanocyl PLASTICYL™ PP2001 Polypropylene - Carbon Nanotube Masterbatch
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Carbon Fiber Filled

Material Notes: PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLASTICYL™ PP2001 is a conductive masterbatch based on polypropylene. Because of its low viscosity and high flow formulation, PLASTICYL™ PP2001 is ideal for standard injection molding and extrusion processes.

Key Applications:

  • ESD (Electrostatic Discharge) and electrically conductive parts
  • E&E automotive and industrial
  • Injection molding, extrusion

Benefits:

  • Electrical conductivity at low loading
  • Retention of key mechanical properties
  • Easier processing

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.872 g/cc0.872 g/ccISO 1183
Filler Content 19 - 21 %19 - 21 %Carbon Nanotube Loading
 
Thermal PropertiesMetricEnglishComments
Melting Point 165 °C329 °FISO 11357-1,-3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polypropylene, Carbon Fiber Filled
Nanocyl EPOCYL™ NC R2HM-01 Formulated Epoxy-Carbon Nanotube Pre-preg Resin System
Overview of materials for Polypropylene with 10% Glass Fiber Filler
NanoAmor 50% Regular Single Walled Carbon Nanotubes
NanoAmor 20% DWNT Double Walled Carbon Nanotubes

PNANOCY973 / 108928

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.