MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Arla SAPHIR® AS PC Sheet
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Extruded

Material Notes: SAPHIR® is a range of polycarbonate coated sheet. SAPHIR® AS, is an antistatic coated polycarbonate sheet with a unique protection against electrostatic charging. SAPHIR® AS is a polycarbonate sheet with a two side anti-static coating. The coating gives an effective protection against electrostatic charging and prevents dust and dirt attraction. SAPHIR® AS prevents electrostatic discharge (ESD) and the high impact strength of polycarbonate is combined with excellent fire properties and optical clarity. SAPHIR® AS is to be used in flat applications.

Benefits: Protection against electrostatic charging; Prevent dust and dirt attraction; Impact Resistant; More than 10 times the impact strength of high impact PMMA

Application: SAPHIR® AS is suitable for hoods and inspection glazing for testing equipment. In applications where it is important to prevent electrostatic build up, such as explosive atmospheres.

Information provided by Arla Plast.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ISO 1183
Moisture Absorption 0.150 %
@Time 86400 sec
0.150 %
@Time 24.0 hour
50% RH; ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 70.0 MPa10200 psiISO 527
Tensile Strength, Yield 60.0 MPa8700 psiISO 527
Elongation at Break 110 %110 %ISO 527
Elongation at Yield 6.0 %6.0 %ISO 527
Modulus of Elasticity >= 2.30 GPa>= 334 ksiISO 527
Flexural Modulus >= 2.30 GPa>= 334 ksiISO 178
Izod Impact, Notched (ISO)  10.0 kJ/m²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 180/1A
 65.0 kJ/m²
@Temperature 23.0 °C
30.9 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
Charpy Impact Unnotched NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
ISO 179/1eU
Charpy Impact, Notched 1.10 J/cm²
@Temperature -30.0 °C
5.23 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Surface Resistance >= 1.00e+8 ohm>= 1.00e+8 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear 65.0 µm/m-°C
@Temperature 20.0 - 70.0 °C
36.1 µin/in-°F
@Temperature 68.0 - 158 °F
ISO 11359-2
Thermal Conductivity 0.200 W/m-K1.39 BTU-in/hr-ft²-°FDIN 8302
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5861.586ISO 489
 
Descriptive Properties
ColorClear (slightly blue)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PARLA941 / 301119

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.