MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Polynt V 322 HF Putty
Categories: Polymer; Thermoset; Vinyl Ester

Material Notes: V 322 HF is a general purpose EPOXY VINYL ESTER bonding putty with fire retardant properties. Suitable for fiberglass bonding where improved toughness, environmental resistance and fire retardant properties may be required.

Features And Benefits:

  • V 322 HF is easy to apply by using an appropriate tools such as spatula or a trowel
  • Recommended for use a methyl ethyl ketone peroxide (MEKP) catalyst
  • Excellent bonding with fiber glass parts.
  • Available in 20 liters pails and 205 liters drums.

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Brookfield Viscosity 350000 - 400000 cP350000 - 400000 cPRVF #7 @ 5 rpm
 
Processing PropertiesMetricEnglishComments
Gel Time 6.00 - 10.0 min
@Temperature 25.0 °C
6.00 - 10.0 min
@Temperature 77.0 °F
1% MEC EX tested @ 25°C in 100 g mass
Shelf Life 1.50 Month1.50 Month
 
Descriptive Properties
Thixotropic Index>6

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLYN9022 / 231617

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.